Thermal Properties Metric English Comments
Melting Point 1750 - 1765 °C
3180 - 3209 °F
Johnson Matthey HC Platinum w/ 5% Cobalt Jewelry Alloy
Fluid for hard castings. Cobalt has been used to create casting alloys at various levels of fineness. Cobalt suppresses oxygen level in the melt, improves fluidity and castability and gives a good ..
Melting Point 1755 - 1765 °C
3191 - 3209 °F
Johnson Matthey SC 950 Platinum w/ 5% Palladium Jewelry Alloy
Castings, delicate settings. Palladium has been used to create casting alloys at various levels of fineness. Palladium produces a softer casting.
Melting Point 1750 - 1765 °C
3180 - 3209 °F
Wieland 1746 Wilaform Platinum
Platinum alloy particularly suitable for decoration castingApplications: casting, laminar decoration, tubingDental