Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1005 - 1080 °C | 1841 - 1980 °F | |
Kennametal Stellite Deloro® 15 Nickel Alloy Deloro™ 15 is a pre-alloyed gas atomized nickel-based powder which is used primarily for the local repair of cast iron glass forming molds. It has excellent weld characteristics and is a good c.. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
IBC Advanced Alloys C17510 Beryllium Copper Alloy Rounds, Temper A(TB00) C17510 - Beryllium Copper mold alloys have hardnesses comparable to tool steel, but with superior thermal conductivity. Beryllium copper plate, block, bar and rounds -- upset forged and heat treated.. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
IBC Advanced Alloys C17510 Beryllium Copper Alloy Rounds, Temper AT(TF00) C17510 - Beryllium Copper mold alloys have hardnesses comparable to tool steel, but with superior thermal conductivity. Beryllium copper plate, block, bar and rounds -- upset forged and heat treated.. |
|||
Melting Point | 1070 - 1080 °C | 1950 - 1980 °F | |
IBC Advanced Alloys C18150 Chrome Copper Zirconium Alloy, TL06 Temper C18150 Chrome Copper Zirconium is recommended for spot and seam welding cold and hot-rolled steel, stainless steel and low conductivity brass and bronze. C18150 Chrome Copper Zirconium Alloy is typi.. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Beryllium Copper Alloy 3 Forgings & Extrusions; AT (TF00) Temper (UNS C17510) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17510) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; HT (TH04) Temper; up to 76 mm Thickness (UNS C17510) Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Beryllium Copper Alloy 3 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Beryllium Copper Alloy 3 Rod and Bar; AT (TF00) Temper; All Sizes (UNS C17510) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Beryllium Copper Alloy 3 Rod and Bar; H (TD04) Temper; up to 76 mm (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Beryllium Copper Alloy 3 Rod and Bar; HT (TH04) Temper; up to 76 mm (UNS C17510) Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Beryllium Copper Alloy 3 Wire; A (TB00) Temper; 1.3-12.7 mm Diameter (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Brush 1915â„¢ Hard Temper Wire, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Brush 1915â„¢ Annealed Temper Wire Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Brush 1915™ Heat Treated Temper Wire, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee.. |
|||
Melting Point | 1030 - 1080 °C | 1890 - 1980 °F | |
Materion Brush 60™ 3/4 HT Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation afte.. |
|||
Melting Point | 977 - 1080 °C | 1790 - 1970 °F | |
Universal Wire Works BNi-1 (AMS 4775) Nickel Base Brazing Filler Metal Information provided by Universal Wire Works for their line of welding wire and filler metal. |
|||
Melting Point | 1020 - 1080 °C | 1870 - 1980 °F | |
Wieland 1911 Wilaform Gold Hard palladium white gold alloy with beautiful white color.Applications: casting, chains, laminar decoration, pipes, tubingDental |
|||
Melting Point | 1075 - 1080 °C | 1967 - 1980 °F | |
CMW® 328 Copper Alloy CMW® 328 material is a high strength, high conductivity copper base alloy. CMW® 328 is heat treatable. Optimum mechanical and physical properties of CMW® 328 material are developed by heat treatm.. |
|||
Melting Point | 980.0 - 1080 °C | 1796 - 1976 °F | |
Cadi 150 Copper Alloy A small addition of Zr to copper improves resistance to softening and resists deformation at high temperatures where normal copper would soften rapidly. Zirconium copper is used as a Class 1 electr.. |
|||
Melting Point | 1070 - 1080 °C | 1958 - 1976 °F | |
Cadi 182 Copper Alloy Chromium copper is the primary copper alloy used for resistance spot and seam welding. This alloy achieves good hardness and electrical conductivity through a combination of heat treatment and cold .. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Beryllium Copper Alloy 3 Tube; H (TD04) Temper; up to 76 mm o.d. (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Beryllium Copper Alloy 3 Tube; HT (TH04) Temper; up to 76 mm o.d. (UNS C17510) Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc... |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Beryllium Copper Alloy 3 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17510) Treatment required for max strength: 3 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials .. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Beryllium Copper Alloy 3 Wire; H (TD04) Temper; 1.3-12.7 mm Diameter (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; H (TD04) Temper; up to 76 mm Thickness (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Beryllium Copper Alloy 3 Strip; HT (TH04) Temper (UNS C17510) Treatment required for max strength: 2-3 hrs @ 480ºC or Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 75%Formability Ratio.. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Beryllium Copper Alloy 3 Tube; A (TB00) Temper; All Sizes (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 1040 - 1080 °C | 1900 - 1980 °F | |
Materion Beryllium Copper Alloy 3 Tube; AT (TF00) Temper; All Sizes (UNS C17510) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc... |