Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 68.0 °C | 154 °F | Exxon Method |
ExxonMobil Escorene® UL-7740 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Melting Point | 68.0 °C | 154 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5005 1000 Micron EVA Powder Description: ICOFLO 510-5005 is an EVA powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in masterbatch (inste.. |
|||
Melting Point | 68.0 °C | 154 °F | DSC; ASTM D3418 |
ICO Polymers ICOTEXâ„¢ 520-5005 1000 Micron EVA Powder Description: ICOTEX 520-5005 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: very high melt flow, fast melting, great .. |
|||
Melting Point | 68.0 - 72.0 °C | 154 - 162 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 102 Linear Thermoplastic Polyurethane PEARLBOND® 102 is a linear, polycaprolactone-based polyurethane, supplied in form of small white pellets, which combines a very high crystallization rate with a very high thermoplasticity level.A.. |
|||
Melting Point | 68.0 - 72.0 °C | 154 - 162 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 502 Linear Thermoplastic Polyurethane PEARLBOND™ 502 is a linear, polycaprolactone-copolyester polyurethane with a high crystallization rate and a very high thermoplasticity level.Application: Pearlbond™ 502 can be added to fo.. |
|||
Melting Point | 68.0 °C | 154 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Elvax® 3165 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 18 wt% Vinyl Acetate.Elvax® 3165 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melting Point | 68.0 °C | 154 °F | Freezing Point; ASTM D3417 |
DuPont Elvax® 3165LG Ethylene Vinyl Acetate DuPont™ Elvax® 3165XZ is an extrudable ethylene-vinyl acetate copolymer resin containing low gel material available in pellet form for use in conventional extrusion equipment designed to process p.. |
|||
Melting Point | 68.0 °C | 154 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Elvax® 3165SB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 18 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Melting Point | 68.0 °C | 154 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Elvax® 3170 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 18 wt% Vinyl Acetate.Elvax® 3170 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melting Point | 68.0 °C | 154 °F | Freezing Point; ASTM D3418, ISO 3146 |
DuPont™ Elvax® 3169Z Ethylene Vinyl Acetate DuPont™ Elvax® 3169Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 3.. |
|||
Melting Point | 68.0 °C | 154 °F | Dow Method |
Dow AFFINITY™ GA 1900 Polyolefin Plastomer (POP) AFFINITY™ GA 1900 Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. This product can be used in applications such as polymer modification (i.e. flow enhancement and.. |
|||
Melting Point | 68.0 °C | 154 °F | DSC |
Arkema Group OREVAC® 9305 EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Melting Point | 68.0 °C | 154 °F | DSC |
Arkema Group EVATANE® 28-150 Copolymer Ethylene - Vinyl Acetate EVATANE® 28-150 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-150 is stabilized with antioxidants. The High Vinyl Acetate .. |
|||
Melting Point | 68.0 °C | 154 °F | Freezing Point; ASTM D3417 |
DuPont Elvax® 3165Z Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 3165Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additives.. |
|||
Melting Point | 68.0 °C | 154 °F | Freezing Point; ASTM D3417 |
DuPont Elvax® 3172Z Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 3172Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additives.. |
|||
Melting Point | 68.0 °C | 154 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Elvax® 3169 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
(discontinued **) 18 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Melting Point | 68.0 °C | 154 °F | Freezing Point; ASTM D3417 |
DuPont Elvax® 3550SBH Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 3550SBH is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additiv.. |