Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 325 °C | 617 °F | ASTM D570 |
Solvay Specialty Polymers Amodel® A-1133 NL WH 886 Polyphthalamide (PPA)
(discontinued **) Amodel A-1133 NL WH 886 resin is a glass reinforced polyphthalamide (PPA ) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib.. |
|||
Melting Point | 325 °C | 617 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AE-8133 Polyphthalamide (PPA)
(discontinued **) Amodel AE-8133 is a 33% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temperature, high flexural.. |
|||
Melting Point | 325 - 330 °C | 617 - 626 °F | ISO.3146 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Melting Point | 325 - 330 °C | 617 - 626 °F | |
Solvay Specialty Polymers Polymist® F-5A EX PTFE Powder Lubricant
(Unverified Data**) Polymist® powders are a family of white free-flowing polytetrafluoroethylene powders for use as additives in other materials to enhance processing or end-use performance characteristics. Polymist .. |
|||
Melting Point | 325 - 330 °C | 617 - 626 °F | |
Solvay Specialty Polymers Polymist® F-510 PTFE Powder Lubricant
(discontinued **) Polymist® powders are a family of white free-flowing polytetrafluoroethylene powders for use as additives in other materials to enhance processing or end-use performance characteristics. Polymist .. |
|||
Melting Point | 325 - 335 °C | 617 - 635 °F | |
Isoflon Virgin PTFE Polytetrafluoroethylene Properties/Improved compression and wear resistanceExcellent chemical stabilityBetter thermal conductivityExcellent resistance to continuous service temperatures up to 260°C, and, for limited per.. |
|||
Melting Point | 325 - 335 °C | 617 - 635 °F | ASTM D3418 |
Solvay Specialty Polymers Algoflon® L101 Polytetrafluoroethylene (PTFE) Algoflon® L101 a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L101 can be de-agglomerated.. |
|||
Melting Point | 325 - 335 °C | 617 - 635 °F | ASTM D3418 |
Solvay Specialty Polymers Algoflon® L203F Polytetrafluoroethylene (PTFE) Algoflon® L203F a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L203F can be de-agglomerat.. |
|||
Melting Point | 325 - 335 °C | 617 - 635 °F | ASTM D3418 |
Solvay Specialty Polymers Algoflon® L206 Polytetrafluoroethylene (PTFE) Algoflon® L206 a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L206 can be de-agglomerated.. |
|||
Melting Point | 325 - 335 °C | 617 - 635 °F | ASTM D3418 |
Solvay Specialty Polymers Algoflon® L206F Polytetrafluoroethylene (PTFE) Algoflon® L206F a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L206F can be de-agglomerat.. |
|||
Melting Point | 325 °C | 617 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AE-8950 Polyphthalamide (PPA), 50% Glass Fiber Amodel® AE-8950 is a 50% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep .. |
|||
Melting Point | 325 - 335 °C | 617 - 635 °F | ASTM D3418 |
Solvay Specialty Polymers Algoflon® L203 Polytetrafluoroethylene (PTFE) Algoflon® L203 a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L203 can be de-agglomerated.. |
|||
Melting Point | 325 °C | 617 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® A-8950 HS Polyphthalamide (PPA), 50% Glass Fiber Amodel® A-8950 HS is a 50% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance, low mo.. |
|||
Melting Point | 325 °C | 617 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HTV-3H1 black 9205 PA6T/6I-GF30 Product description: Grivory HTV-3H1 black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Melting Point | 325 °C | 617 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HTV-5H1 black 9205 PA6T/6I-GF50 Product description: Grivory HTV-5H1 black 9205 is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Melting Point | 325 °C | 617 °F | ISO 3146 |
ExxonMobil PP8013L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with very high impact strength at low temperature. It is suitable for molding applications like containers and tubs, other rigid packaging, t.. |
|||
Melting Point | 325 °C | 617 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HT1V-4 FWA black 9225 PA6T/6I-GF40 Product description: Grivory HT1V-4 FWA black 9225 is a 40 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Melting Point | 325 °C | 617 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HT1V-45 HY black 9205 PA6T/6I-GF45 Product description: Grivory HT1V-45 HY black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-45 HY .. |
|||
Melting Point | 325 °C | 617 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HT1V-5 HY black 9205 PA6T/6I-GF50 Product description: Grivory HT1V-5 HY black 9205 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-5 HY bl.. |
|||
Melting Point | 325 °C | 617 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HTV-5H1 nat PA6T/6I-GF50 Product description: Grivory HTV-5H1 natural is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
Melting Point | 325 °C | 617 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HT1V-4 FWA nat PA6T/6I-GF40 Product description: Grivory HT1V-4 FWA natural is a 40 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6.. |
|||
Melting Point | 325 °C | 617 °F | |
Asahi Glass Fluon® L150J PTFE Lubricant Fluon®PTFE lubricants are used as additive to plastics, rubbers, paints, greases and so on. Frictional resistance decreases and non-stick increases on the applied surface.Information provided by As.. |
|||
Melting Point | 325 °C | 617 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® A-1422 LS WH 171 Polyphthalamide (PPA)
(discontinued **) Amodel A-1422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature range, .. |
|||
Melting Point | 325 °C | 617 °F | |
Solvay Specialty Polymers Amodel® AFA-4133 V0 Z Polyphthalamide (PPA), Dry
(discontinued **) Amodel AFA-4133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |