Solvay Specialty Polymers Algoflon® L203 Polytetrafluoroethylene (PTFE)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , PTFE Powder
Manufacturer Solvay Specialty Polymers
Trade Name Algoflon®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Solvay Specialty Polymers Algoflon® L203 Polytetrafluoroethylene (PTFE).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Algoflon® L203 a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L203 can be de-agglomerated to sub-micron particle size by the application of shear providing a better dispersion and distribution of the PTFE particles in the application. Designed for use in critical engineering and high end performance lubricants to improve thickening effect, lubricity, Algoflon® L203 improves also corrosion and temperature resistance.Uses: AdditiveAdditional Properties: Average Particle Size - Internal Method 5.0 µm; Bulk Density - ASTM D3418 325 g/l; Specific Surface Area - Internal Method > 7.5 m²/gInformation provided by Solvay Specialty Polymers.
Thermal Properties Metric English Comments
Melting Point 325 - 335 °C
617 - 635 °F
ASTM D3418
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
Color White
Form Powder