Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 227 °C | 440 °F | ASTM D3418 |
Nylene® Vexel™ B12GF15 , 15% Glass Reinforced PBT Description: Vexel™ B12GF15 is a 15% glass fiber reinforced, general purpose PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeri.. |
|||
Melting Point | 227 °C | 440 °F | ASTM D3418 |
Nylene® Vexel™ B12GF15 SA , 15% Glass Reinforced PBT Description: Vexel™ B12GF15 SA is a 15% glass fiber reinforced PBT with improved surface aPolyphenylene Etherarance. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are.. |
|||
Melting Point | 227 °C | 440 °F | ASTM D3418 |
Nylene® Vexel™ B12GF30 , 30% Glass Reinforced PBT Description: Vexel™ B12GF30 is a 30% glass fiber reinforced, general purpose PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeri.. |
|||
Melting Point | 227 °C | 440 °F | ASTM D3418 |
Nylene® Vexel™ B12GF30 FR , 30% Glass Reinforced, Flame Retardant PBT Description: Vexel™ B12GF30 FR is a 30% glass fiber reinforced, flame retardant PBT. B12GF30 FR is UL approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all .. |
|||
Melting Point | 227 °C | 440 °F | ASTM D3418 |
Nylene® Vexel™ B12GF30 SA , 30% Glass Reinforced PBT Description: Vexel™ B12GF30 SA is a 30% glass fiber reinforced PBT with improved surface aPolyphenylene Etherarance. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are.. |
|||
Melting Point | 227 °C | 440 °F | ASTM D3418 |
Nylene® Vexel™ B12GF45 , 45% Glass Reinforced PBT Description: Vexel™ B12GF45 is a 45% glass fiber reinforced, general purpose PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeri.. |
|||
Melting Point | 227 °C | 440 °F | ASTM D3418 |
Nylene® Vexel™ B12U FR Un-reinforced, Flame Retardant PBT Description: Vexel™ B12U FR is an un-reinforced, flame retardant PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources .. |
|||
Melting Point | 227 °C | 440 °F | ASTM D3418 |
Nylene® Vexel™ B50U , High Flow, Un-reinforced PBT Description: Vexel™ B50U is a high flow, un-reinforced PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporatio.. |
|||
Melting Point | 227 °C | 441 °F | ISO 11357-1,-3 |
Nanocyl PLASTICYL™ PBT1501 Polybutylene Terephthalate - Carbon Nanotube Masterbatch PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Melting Point | 227 - 310 °C | 441 - 590 °F | |
Nihon Superior SN100C3 High Temperature Dipper and Tinning Solder High temperature dip soldering and tinning of copper wire, polyurethane coated wire and component terminations. For use at up to 400°C. |
|||
Melting Point | 227 - 340 °C | 441 - 644 °F | |
Nihon Superior SN100C4 High Temperature Dipper and Tinning Solder High temperature dip soldering and tinning of copper wire, polyurethane coated wire and component terminations. For use at up to 400°C. |
|||
Melting Point | 227 °C | 441 °F | |
Nihon Superior SN100CL Lead-Free Solder Alloy Used for hot air solder leveling (HASL). Features include: Excellent fluidity; Bridge-free coating of the fine pitch circuitry; Bright smooth and uniform coating; Low copper erosion; Formation of st.. |
|||
Melting Point | 227 °C | 441 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Sorona® 3015GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3015GV NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |
|||
Melting Point | 227 °C | 441 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Sorona® FG3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data** Sorona® FG3015G NC010 is a 15% glass fiber reinforced polytrimethylene terephthalate resin containing 31% renewably sourced ingredients by weight (37% based on polymer only) formulated to be food c.. |
|||
Melting Point | 227 °C | 441 °F | Eutectic |
Indium Corp. Indalloy® 244 99.3Sn/0.7Cu Lead-Free Solder Alloy Inexpensive. Alloy of choice for general wave solder assembly.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 227 °C | 441 °F | Eutectic |
Indium Corp. Indalloy® 262 Tin-Copper Solder Alloy Information provided by the manufacturer, Indium Corporation of America. |
|||
Melting Point | 227 °C | 441 °F | DSC |
Solvay Specialty Polymers Halar® 2408DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE), Filled Halar® 2408DA is a filled, pearl-white, semicrystalline melt processable fluorinated resin that may be used in full compliance with the federal Food, Drug, and Cosmetic Act. It is designed for el.. |
|||
Melting Point | 227 °C | 441 °F | DSC |
Solvay Specialty Polymers Halar® 2508DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® 2508DA is a filled, black, semi-crystalline melt processable fluorinated resin that may be used in full compliance with the Federal Food, Drug and Cosmetic Act. It is designed for electros.. |
|||
Melting Point | 227 °C | 441 °F | DSC |
Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Melting Point | 227 °C | 441 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Sorona® 3015GV BK001 Polytrimethylene Terephthalate (PTT) 15% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3015GV BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (37% based .. |
|||
Melting Point | 227 °C | 441 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Sorona® 3015GV NC010 Polytrimethylene Terephthalate (PTT) 15% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3015GV NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% based on pol.. |
|||
Melting Point | 227 °C | 441 °F | ASTM D789 |
Diamond Polymers NYLON 6001GF33 33% Glass Filled Polyamide Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melting Point | 227 - 238 °C | 440 - 460 °F | |
Cast Nylons Nycast® GX Solid Lubricant Filled Gray Cast Nylon 6 NYCAST® GX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti.. |
|||
Melting Point | 227 °C | 441 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Sorona® 2045G BK346A Polytrimethylene Terephthalate (PTT)
(Unverified Data**) 45% Glass Reinforced Polytrimethylene TerephthalateInformation provided by DuPont Performance Polymers |
|||
Melting Point | 227 °C | 441 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Sorona® FG3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data** 15% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Developed for Food Contact Applications Sorona FG3015G NC010 is a 15% glass fiber reinforced polytrimethylene terephthalate resi.. |
|||
Melting Point | 227 °C | 441 °F | ASTM D3418 |
Custom Resins Vexel™ 4200 RD PBT; 30% Glass Filler
(discontinued **) Property data for dry as molded samples.Data provided by the manufacturer |
|||
Melting Point | 227 °C | 441 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Sorona® 3015G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3015G BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |
|||
Melting Point | 227 °C | 441 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness a.. |
|||
Melting Point | 227 °C | 441 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |
|||
Melting Point | 227 - 229 °C | 441 - 444 °F | Average value: 227 °C Grade Count:16 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |