Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Hytrel® HTR8730 BK320 TPC-ET
(Unverified Data**) Hytrel® HTR8730 BK320 is a high viscosity thermoplastic polyester elastomer designed for blow molding. It has excellent mechanical properties at elevated temperatures and very good resistance to mo.. |
|||
Melting Point | 212 - 280 °C | 414 - 536 °F | Average value: 257 °C Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Unfilled". Each property range of values reported is minimum and maximum v.. |
|||
Melting Point | 212 °C | 414 °F | Peak |
LG Chemical KEYFLEX BT 1063D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1, -3 |
Lanxess Durethan® BKV 115 H3.0 000000 Nylon 6-Copolymer, Glass Fiber Reinforced PA 6-Copolymer, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® C 38 FA 000000 Copolyamide Copolyamide, film quality, high transparency, with slip agent, not nucleatedApplication Examples: blown film coextrusion (central layer) |
|||
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® C 38 FKAM 000000 Copolyamide Copolyamide, film quality, high transparency, nucleated, high slip and lubricant content, medium-viscosity, good antiblock and dynamic slip propertiesApplication Examples: blown film coextrusion (ou.. |
|||
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® C 38 FKS 000000 Copolyamide Copolyamide, film quality, high transparency, with processing aid, nucleatedApplication Examples: blown film coextrusion (outer layer) |
|||
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® C 38 F 000000 Copolyamide PA 6-Copolymer, non-reinforced, extrusion, medium viscosity, no additives, high transparency |
|||
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1, -3 |
Lanxess Durethan® C 38 FAM 000000 Copolyamide PA 6-Copolymer, non-reinforced, extrusionInformation provided by LANXESS. |
|||
Melting Point | 212 °C | 414 °F | By DSC |
Toyobo PELPRENE™ P150B Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Melting Point | 212 °C | 414 °F | ISO 3146 |
Chengdu Polyster H6555 Thermoplastic Polyether-ester Elastomer (TPEE) Medium modulus molding and extrusion grade. Contains improved color- stable antioxidants. Good balance of modulus and toughness. Parts and components of automobile, hydraulic hose and slide of eleva.. |
|||
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® EM630 63 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® EM630 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® EM631-HB TPC-ET Extrusion Grade, Heat Stabilized |
|||
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® PB420-B TPC-ET Blow Molding Grade |
|||
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® PL380 38 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® PL380 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® PL381-H TPC-ET Injection Molding |
|||
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® PM381 38 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® PM381 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® VT3104 TPC-ET Extrusion Grade |
|||
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® EL630 63 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Hytrel® HTR8730 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Viscosity Polyester Elastomer with Excellent Mechanical Properties at Elevated Temperatures Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Melting Point | 212 °C | 414 °F | ISO 3146 |
Cathay PA511 Renewable Engineering Polyamide Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr.. |
|||
Melting Point | 212 °C | 414 °F | ASTM D3418 |
Ashley Polymers Ashlene® 980LS-33G Nylon 612, 33% Glass Reinforced A 33% glass reinforced, heat stabilized Nylon 612 resin.Data provided by the manufacturer |
|||
Melting Point | 212 °C | 414 °F | ASTM D3418 |
Ashley Polymers Ashlene® 980LS-40G Nylon 612, 40% Glass Reinforced A 40% glass reinforced, heat stabilized Nylon 612 resin.Data provided by the manufacturer |
|||
Melting Point | 212 °C | 414 °F | ASTM D3418 |
Ashley Polymers Ashlene® 980LS-43GB Nylon 612, 43% Glass Reinforced A 43% glass reinforced, heat stabilized Nylon 612 resin in black.Data provided by the manufacturer |
|||
Melting Point | 212 °C | 414 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® EL630 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |