Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 202 °C | 396 °F | ASTM D3418 |
SK Chemicals SKYPEL G155D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Melting Point | 202 °C | 396 °F | ASTM D3418 |
SK Chemicals SKYPEL M555DH General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Melting Point | 202 °C | 396 °F | |
Sanyo PELESTAT® NC6321 Antistatic Additive PELESTAT® alloy type anti-static additives are true IDP (Inherent Dissipative Polymers) that give permanent static dissipation performance to thermoplastics. Pelestat® comes tailored to a var.. |
|||
Melting Point | 202 °C | 396 °F | ASTM D3418 |
SK Chemicals SKYPEL G455D Special Grade Oil-Resistant Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Melting Point | 202 °C | 396 °F | ASTM D3418 |
SK Chemicals SKYPEL P137DW Productivity Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Melting Point | 202 °C | 396 °F | ISO 11357-3 |
Suzhou Hipro Polymers Hiprolon® 11 PFB Colorized Nylon powder Hiprolon® 11 PFB colorized is a fluid-bed polyamide powder fully comprised of bio-renewable raw materials. It has excellent weather ability, chemical resistance, wear resistance, impact resistanc.. |
|||
Melting Point | 202 °C | 396 °F | ISO 11357 |
Suzhou Hipro Polymers Hiprolon® 200 MC HLS G30 Nylon 1010, 30% glass fiber filled Hiprolon® 200 MC HLS G30 is a polyamide 10.10 compound reinforced with 30% chopped glass fiber for injection molding; features high dimension stability, chemical resistance, impact resistance, lo.. |
|||
Melting Point | 202 °C | 396 °F | ISO 11357 |
Suzhou Hipro Polymers Hiprolon® 200 NN Nylon 1010, conditioned Hiprolon® 200 NN is a medium viscosity polyamide 10,10 with neat resin based on bio-renewable resource. It features low density, low water absorption, good cold impact resistance, good wear-resi.. |
|||
Melting Point | 202 °C | 396 °F | ISO 11357-1/-2 |
Suzhou Hipro Polymers Hiprolon® 200 NN Nylon 1010, dry Hiprolon® 200 NN is a medium viscosity polyamide 10,10 with neat resin based on bio-renewable resource. It features low density, low water absorption, good cold impact resistance, good wear-resi.. |
|||
Melting Point | 202 °C | 396 °F | ISO 11357-3 |
Suzhou Hipro Polymers Hiprolon® 211 PES Colorized Nylon powder Hiprolon® 211 PES colorized electrostatic polyamide powder is fully comprised of bio-renewable raw materials. It has excellent weather ability, chemical resistance, wear resistance, impact resist.. |
|||
Melting Point | 202 °C | 396 °F | |
Eastman Ecdel PCCE 9966 Copolyester Ether Elastomer ISO data as provided by the manufacturer, Eastman Chemical |
|||
Melting Point | 202 °C | 396 °F | |
Esstech X-801-0000 d, I - Camphorquinone, C10H14O2 CQ or camphorquinone is a visible light-activated initiator commonly used in UDMA systems. Listed on the Toxic Substance Control Act List. CAS # 10373-78-1.Information provided by ESSTECH, Inc. |
|||
Melting Point | 202 °C | 396 °F | |
BASF AH-Salt Recommended use: For the production of homopolymerisates and copolymerisatesInformation provided by BASF |