Thermal Properties Metric English Comments
Melting Point 200 - 220 °C
392 - 428 °F
DSC; STN EN ISO 3146
Plastcom SLOVASTER® B GF 20 FRK 3 Polybutylene Terephthalate, 20% Chemically Coupled Glass Fiber, Red Phosphorus Flame Retardant
FeaturesPBT with the content of 20% chemically coupled glass fiber and flame retardant based on red phosphorus. Anisotropy of shrinkage enables injection moulding of round, cylindrical or other hol..
Melting Point 200 - 220 °C
392 - 428 °F
DSC; STN EN ISO 3146
Plastcom SLOVASTER® B GF 30 FRK 3 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Red Phosphorus Flame Retardant
FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on red phosphorus. Anisotropy of shrinkage enables injection moulding of round, cylindrical or other hol..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B1 GF 20 000/2 PBT, 20% glass fibre
FeaturesPBT for injection moulding, pure without lubricant, chemically reinforced with 20% glass fibre, excellent flow. Characterised by excellent properties also at minus temperatures like eg. modu..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B1 GF 45 PBT, 45% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 45% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Melting Point 200 - 220 °C
392 - 428 °F
STN EN 11357-1
Plastcom SLOVASTYR® B BT N PBT
Regranulate PBT basic type for injection molding. Melt is characterized by very good fluidity, which enables injection molding of complicated and divided products also on multiple moulds. Anisotropy..
Melting Point 200 - 250 °C
392 - 482 °F
Average value: 224 °C Grade Count:18
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B GB 20 M PBT, 20% glass beads
FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B1 GF 10 MI PBT, 10% glass fibre
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B1 HML GF 10 PBT, 10% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Melting Point 200 - 260 °C
392 - 500 °F
Average value: 234 °C Grade Count:3
Overview of materials for Nylon 66/6, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl..
Melting Point 200 °C
392 °F
ASTM D3418
Honeywell Aegis™ HCA73MP Nylon 6/6,6 Extrusion Grade Copolymer  (discontinued **)
Description: Aegis HCA73MP is a lubricated and nucleated low viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 C..
Melting Point 200 °C
392 °F
ASTM D3418
Honeywell Aegis™ HCA73ZP Nylon 6/6,6 Extrusion Grade Copolymer  (discontinued **)
Description: Aegis HCA73ZP is a low viscosity nylon 6/6,6 copolymer extrusion grade. It conforms to Food and Drug Administration requirements of 21 CFR177.1500. Aegis HCA73ZP possesses the combinati..
Melting Point 200 °C
392 °F
ASTM D3418
Honeywell Aegis™ HCA155MP Nylon 6/6,6 Extrusion Grade Copolymer  (discontinued **)
Description: Aegis HCA115MP is a lubricated and nucleated high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21..
Melting Point 200 °C
392 °F
Peak
LG Chemical KEYFLEX BT 2140D Ester Type TPE
Description: Injection Molding, TPC-ET, Specialty, Low ModulusApplication: Films & SheetsCAS: 37282-12-5Information provided by LG Chemical
Melting Point 200 - 220 °C
392 - 428 °F
ISO R 1218
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Dry
Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH
Melting Point 200 °C
392 °F
ASTM D2117
Samyang Triel® 5401BM Thermoplastics Polyetherester Elastomer, Blow Molding
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5401BM is for blow molding applications.Applications: Automotive - CVJB and BellowsInformation provided ..
Melting Point 200 °C
392 °F
By DSC
Toyobo PELPRENE™ S1002 Polyester TPE, Ultra Heat-resistant
Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo.
Melting Point 200 °C
392 °F
10°C/min; ISO 11357-1/-3
DSM Novamid® 2030 FC PA666
Film Extrusion, Extrusion, Extrusion Grade
Melting Point 200 °C
392 °F
10°C/min; ISO 11357-1/-3
EMS-Grivory Grivory® 1SBVX-30H LDS black PA1010-GF30
Product Description: Grilamid 1SBVX-30H LDS black is a 30% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring techno..
Melting Point 200 °C
392 °F
10°C/min; ISO 11357-1/-3
DSM Novamid® 2030A PA666
Film Extrusion, Extrusion, Extrusion Grade
Melting Point 200 °C
392 °F
10°C/min; ISO 11357-1/-3
EMS-Grivory Grivory® 1SVX-50H black 9288 PA1010-GF50
Product Description: Grilamid 1SVX-50H black 9288 is a 50% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile. Key properties of Grilamid 1SBVX-50H LDS ..
Melting Point 200 °C
392 °F
10°C/min; ISO 11357-1/-3
DSM Novamid® 2030CA FC PA666
Film Extrusion, Extrusion, Extrusion Grade
Melting Point 200 °C
392 °F
10°C/min; ISO 11357-1/-3
EMS-Grivory Grivory® 1SVX-65H nat PA1010-GF65
Product Description: Grilamid 1SVX-65H natural is a 65% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E..
Melting Point 200 °C
392 °F
10°C/min; ISO 11357-1/-3
DSM Novamid® 2030CA PA666
Film Extrusion, Extrusion, Extrusion Grade
Melting Point 200 °C
392 °F
10°C/min; ISO 11357-1/-3
EMS-Grivory Grivory® XE 4116 black 9288 PA1010-GF55
Product description: Grilamid XE 4116 black 9288 is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, paint..
Melting Point 200 °C
392 °F
10°C/min; ISO 11357-1/-3
EMS-Grivory Grivory® XE 4116 nat PA1010-GF55
Product description: Grilamid XE 4116 natural is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, painted ..
Melting Point 200 °C
392 °F
10°C/min; ISO 11357-1/-3
EMS-Grivory Grivory® XE 4174 black 9992 PA1010-GF30
Product description: Grilamid XE 4174 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4174 black 9992 are: PA1010..
Melting Point 200 °C
392 °F
10°C/min; ISO 11357-1/-3
DSM Arnitel® UM551-V 55 Shore D, Flame Retardant (halogen-, phosphorous-free) Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B1 GF 30 PBT, 30% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..