Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® 150 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability, low die deposit, and enhanced crystallization for low porosity.Information pr.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® 327UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 327UVE NC010 (formerly DE20554) is a medium-high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Informat.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® 988PA NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 988PA NC010 is a low viscosity acetal homopolymer for injection molding with low screw deposit. It is especially formulated for gear applications requiring high precision and dimensional st.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG900P is a low viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information prov.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® SC690 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® SC690 is a low viscosity acetal homopolymer, developed for parts requiring high precision molding in the healthcare industry.Information provided by DuPont Performance Polymers |
|||
Melting Point | 178 °C | 352 °F | |
Aardvark Polymers AARTEL® 2100UV Acetal Homopolymer Rotational Molding Resin Aartel 2100UV is a natural acetal homopolymer with UV stabilizers.Aartel 2100UV is a medium viscosity resin with excellent flow characteristics.Aartel 2100UV is available in natural white and may be.. |
|||
Melting Point | 178 °C | 352 °F | ASTM D3418 |
UBE UBESTA® 3014U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Melting Point | 178 °C | 352 °F | ASTM D3418 |
UBE UBESTA® 3020X15 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Melting Point | 178 °C | 352 °F | ASTM D3418 |
UBE UBESTA® 3024U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 20 G grey 9280 PA12 Product Description: Grilamid L 20 G grey 9280 is a medium viscosity, unreinforced, heat stabilized polyamide 12 for injection molding and cable sheathing. The main features of this product are: Low.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 20 G PA12 Product Description: Grilamid L 20 LG is a normal viscosity, heat stabilized polyamide 12 non-reinforced injection molding grade. This product has very good flow characteristics Low moisture absorpt.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 25H FWA nat PA12 Product Description: Grilamid L 25 H FWA natural is a highviscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 25 H FWA natural is designed for technical injection moulded com.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® LM-05 HX nat PA12 Product description: Grilamid LM-05 HX natural is a medium viscosity, heat-stabilized nanocomposite PA12 extrusion and injection molding grade. The special features of Grilamid LM-05 HX natural are:.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® LV-15H nat PA12-GF15 Product description: Grilamid LV-15H is a 15% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptiongood dimension.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® LV-65H FWA nat PA12-GF65 Product description: Grilamid LV-65H FWA natural is a 65 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® LVX-65H SST black 9288 PA12-GF65 Product description: Grilamid LVX-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following .. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® 100TE NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100TE NC010 (formerly DE20580) is a high viscosity toughened acetal homopolymer with very low VOC emissions. Processing met.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® 500T BK602 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T BK602 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® 500TE NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500TE NC010 (formerly DE20560) is a medium viscosity toughened acetal homopolymer with very low VOC emissions. Processing.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® 577 BK000 Acetal (POM)
(Unverified Data**) 20% Glass Filled Medium Viscosity Acetal Homopolymer Delrin 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler with high stiffness low warpage and low creep for sup.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact ApplicationsDelrin FG500TL medium viscosity acetal homopolymer resin containing 1.5%.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® II150E BK602 Acetal (POM) Nucleated High Viscosity Acetal Homopolymer Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® PC691 NC010 Acetal (POM)
(Unverified Data**) Nucleated Low Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC690 is a low viscosity acetal homopolymer developed for parts requiring high precision molding in the health.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 25 LM PA12 Product Description: Grilamid L 25 LM is a heat and UV stabilized nylon 12 grade for tube extrusion. According to DIN 73378 Grilamid L 25 LM corresponds to the type PA 12 HL. Grilamid L 25 LM fulfil.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® 100KM NC000 Acetal (POM)
(Unverified Data**) Kevlar® Modified High Viscosity Acetal Homopolymer with Low Wear and Low FrictionDelrin 100KM is a high viscosity acetal homopolymer resin modified with Kevlar aramid resin. It is designed for appl.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® 100PE NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE NC010 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions... |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer
(Unverified Data**) Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con.. |
|||
Melting Point | 178 °C | 352 °F | |
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® 300CP BK642 Acetal Homopolymer
(Unverified Data**) Delrin® 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of processing and part performance. This black is formulated to mainta.. |