Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 173 - 183 °C | 343 - 361 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLTHANE® 18VT80 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 18VT80 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and superior hydrolysis and microbe resistan.. |
|||
Melting Point | 173 °C | 343 °F | DSC, both heating and cooling speeds of 20°C/min |
Noltex Soarnol® BS3803 Ethylene Vinyl Alcohol Copolymer Modified ET3803; New Stretchable EVOH. Ethylene content 38 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows .. |
|||
Melting Point | 173 °C | 343 °F | DSC, both heating and cooling speeds of 20°C/min |
Noltex Soarnol® ET3808 Ethylene Vinyl Alcohol Copolymer Ethylene content 38 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a.. |
|||
Melting Point | 173 - 181 °C | 343 - 358 °F | |
Indium Corp. Indalloy® 205 In-Pb Solder Alloy Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics.. |
|||
Melting Point | 173 °C | 343 °F | ASTM D3418 |
Kureha KF Polymer 850 PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Melting Point | 173 °C | 343 °F | ASTM D3418 |
Kureha KF Polymer 1000 PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Melting Point | 173 °C | 343 °F | ASTM D3418 |
Kureha KF Polymer 1300 PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Melting Point | 173 °C | 343 °F | ASTM D3418 |
Kureha KF Polymer 2950 PVDF Copolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Melting Point | 173 °C | 343 °F | ASTM D3418 |
UBE UBESTA® 3030JI9L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet DIN73378 PHLYInformation provided by UBE. |
|||
Melting Point | 173 °C | 344 °F | |
Chase Plastics CP Pryme® AH120 Acetal Copolymer, 20% Glass Fiber Reinforced Form: PelletsInformation provided by Chase Plastics. |
|||
Melting Point | 173 - 185 °C | 343 - 365 °F | |
Williams Advanced Alloys WS185 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 173 °C | 343 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 25 W 40 X PA12-I Product Description: Grilamid L 25 W 40 X is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 X is impact modified and heat and UV stabilized. The m.. |
|||
Melting Point | 173 °C | 343 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 22A W 40 X PA12-I Product Description: Grilamid L 22A W 40 X is a flexible plasticized and impact modified heat and light stabilized Polyamide 12 (PA12). The main features of Grilamid L 22A W 40 X are: Good impact st.. |
|||
Melting Point | 173 °C | 343 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 25 W 40 ESD PA12 Product Description: Grilamid L 25 W 40 ESD is a high viscosity, anti-static highly flexible extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 ESD is plasticized and heat stabilized The inh.. |
|||
Melting Point | 173 °C | 343 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 25 W 40 HL X PA12-I Product Description: Grilamid L 25 W 40 HLX is a flexible Polyamide 12 grade with an excellent cold impact strength and heat stability. Grilamid L 25 W 40 HLX is specially suitable for flexible tube.. |
|||
Melting Point | 173 °C | 343 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 25 W 40 NZ PA12-I Product Description: Grilamid L 25 W 40 NZ is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 NZ is impact modified and heat and UV stabilized. The.. |
|||
Melting Point | 173 °C | 343 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 25 W 40 PA12 Product Description: Grilamid L 25 W 40 is a flexible, plasticised, high viscosity extrusion grade of Polyamide 12 (PA12) Grilamid L 25 W 40 is UV and heat stabilized. The main features of Grilamid .. |
|||
Melting Point | 173 °C | 343 °F | (Dry) |
Arkema Group Rilsan® AESN P20 TL Nylon 12, Flexible Grade (Conditioned) Designation ISO 1874-PA12-P,EHL,22-005Flexible grade for overmolding. Available colors: natural and white. Light and heat stabilized. No lubricant.Flexibility. Very good ability to overmold Pebax an.. |
|||
Melting Point | 173 °C | 343 °F | ASTM D3418 |
3M Dyneon™ PVDF 6012/0000 Polyvinylidene Fluoride 3M™ Dyneon™ PVDF 6012/0000 is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, and .. |
|||
Melting Point | 173 °C | 343 °F | ASTM D3418 |
3M Dyneon™ PVDF 6010/0000 Polyvinylidene Fluoride Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical processing industry, wire and cable industry, semiconductor industry,.. |
|||
Melting Point | 173 °C | 343 °F | ASTM D3418 |
3M Dyneon™ PVDF 60512/0000 Polyvinylidene Fluoride
(discontinued **) Polyvinylidenefluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, and.. |