Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 156 - 195 °C | 313 - 383 °F | Average value: 176 °C Grade Count:31 |
Overview of materials for Ethylene Vinyl Alcohol (EVOH) This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Melting Point | 156 °C | 313 °F | DSC |
EVALCA EVAL® G110 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 48 mol % Ethylene.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of the Kuraray product line. |
|||
Melting Point | 156 - 167 °C | 313 - 333 °F | Huntsman/TMA |
Huntsman IROGRAN® A 78 E 4723 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 78 E 4723 is a thermoplastic polyester- polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and high mec.. |
|||
Melting Point | 156 - 160 °C | 313 - 320 °F | DSC |
Solvay Specialty Polymers Hylar® 5000 Polyvinylidene Fluoride (PVDF) Hylar® 5000 is a crystalline high molecular weight powder form of polyvinylidene fluoride (PVDF) specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically .. |
|||
Melting Point | 156 - 161 °C | 313 - 322 °F | |
Shandong Dongyue Shenzhou New Material Co DS201 Polyvinylidene Fluoride Powder Conformable with: Q/DYS 014-2007Polyvinylidene fluoride (PVDF) powder (DS201) PVDF is the homopolymer of vinylidene fluoride, which is excellent chemical corrosion-resistant, high temperature resist.. |
|||
Melting Point | 156 - 165 °C | 313 - 329 °F | 10°C/min; ASTM D3418 |
Shanghai Ofluorine T-1 PVDF for coatings (DF-1) Description: T-1 PVDF for coatings is solid powder, it can mixed with acrylic resin, additive, and become superior performance baking PVDF fluorocarbon coatings. Compared with other grade of PVDF, T.. |
|||
Melting Point | 156 - 160 °C | 313 - 320 °F | DSC |
Solvay Specialty Polymers Hylar® Latex 932 Polyvinylidene Fluoride (PVDF) Hylar® Latex 932 is a stabilized aqueous dispersion that contains approximately 22% by weight of a high molecular weight PVDF polymer (polyvinylidene fluoride) of medium crystallinity. The disper.. |
|||
Melting Point | 156 - 160 °C | 313 - 320 °F | ISO 3146 |
Borealis Borflow™ HL508FB Polypropylene Homopolymer Borflow HL508FB is a polypropylene homopolymer grade intended for fiber applications characterized by narrow molecular weight distribution, controlled rheology, easy processability, optimal product .. |
|||
Melting Point | 156 - 160 °C | 313 - 320 °F | ISO 3146 |
Borealis Borflow™ HL512FB Polypropylene Homopolymer Borflow HL512FB is a polypropylene homopolymer grade intended for fiber applications characterized by narrow molecular weight distribution, controlled rheology, easy processability, optimal product .. |
|||
Melting Point | 156 °C | 313 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 50E571 Anhydride-Modified Polypropylene Adhesive Resin Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E561 and 50E571 are based on polypropylene random copolymers. They are available in pellet form for use in conventional ext.. |
|||
Melting Point | 156 °C | 313 °F | ISO 3146 |
Chengdu Polyster CH4132 Thermoplastic Polyether-ester Elastomer (TPEE) Poly-basic block copolymer. Good compatibility with POM. For blending with POM to improve impact resilience properties.Information provided by Chengdu Polyster Co., Ltd. |
|||
Melting Point | <= 156 °C | <= 313 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ UL 15028CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 15028CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent.. |
|||
Melting Point | <= 156 °C | <= 313 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ UL 15028EM1 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 15028EM1 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agen.. |
|||
Melting Point | <= 156 °C | <= 313 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ UL 40028CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 40028CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent.. |
|||
Melting Point | <= 156 °C | <= 313 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ UL 40028EM1 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 40028EM1 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agen.. |
|||
Melting Point | 156 °C | 313 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Elvamide® 8061 Nylon
(Unverified Data**) Polyamide MultipolymerInformation provided by DuPont Performance Polymers |
|||
Melting Point | 156 °C | 313 °F | ASTM D3418 |
DuPont Performance Polymers Hytrel® G3548L TPC-ET
(Unverified Data**) Hytrel® G3548L is a low modulus grade with nominal hardness of 35D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injec.. |
|||
Melting Point | 156 - 160 °C | 313 - 320 °F | ASTM D3418 |
Solvay Specialty Polymers Hylar® 5000 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Hylar 5000 is a crystalline high molecular weight powder form of polyvinylidene fluoride specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically strong and .. |
|||
Melting Point | 156 - 224 °C | 313 - 435 °F | Average value: 203 °C Grade Count:93 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |