Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 126 °C | 259 °F | Internal method |
Polimeri Europa Flexirene® FH 56 A Butene Copolymer Linear Low Density Polyethylene Flexirene FH 56 A is a butene copolymer with medium density (C4-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Flexirene FH 56 A are characte.. |
|||
Melting Point | 126 °C | 259 °F | Exxon Method |
ExxonMobil Escorene® LL-3113 LLDPE/Hexene Premium High Strength 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |
|||
Melting Point | 126 °C | 259 °F | Exxon Method |
ExxonMobil Escorene® LL-3218 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3218 have outstanding tensile properties as well as stiffness and toughness. These su.. |
|||
Melting Point | 126 °C | 258 °F | ASTM D3417 |
Total Finathene® 2344 HDPE film
(discontinued **) Applications: Trash can liners, merchandise bags, deli wrapInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines. |
|||
Melting Point | 126 °C | 259 °F | ASTM D3417 |
Total Finathene® 3802N Natural HDPE pipe grade
(discontinued **) Applications: Natural gas distribution, extruded pipes, molded fittings, pipe coating, pipe liningInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and .. |
|||
Melting Point | 126 °C | 259 °F | ISO 3146 |
Total Lacqtene® 2006 PBK 35 HDPE pipe, sheet
(discontinued **) LACQTENE® 2006 PBK 35 is a medium density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2006 PBK 35 may be used for pipe extrusion (micro-irriga.. |
|||
Melting Point | 126 °C | 259 °F | ASTM E 794 |
NOVA Chemicals Surpass® RMs341-UG Octene sHDPE Rotational Molding Resin RMs341-UG complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. RMs341.. |
|||
Melting Point | 126 °C | 259 °F | DSC |
LyondellBasell Montell 0300 Polybutene Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenesApplications: packaging industry, minor additive.. |
|||
Melting Point | 126 °C | 259 °F | DSC |
LyondellBasell Montell 0800 Polybutene Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenes, FDA acceptableApplications: concrete carrierMe.. |
|||
Melting Point | 126 °C | 259 °F | DSC |
LyondellBasell Montell 8340 Polybutene-1 Key Features: semi-crystalline low ethylene content random copolymer, miscible with polypropylenes, FDA acceptableApplications: minor additive in a polyethylene peel seal layerMeets FDA requirements.. |
|||
Melting Point | 126 °C | 259 °F | ASTM D2117 |
Lushan H-4 Adhesive Resin for Aluminum Plastic Composite Pipe Adhesive resin Lushan series for aluminum-plastic composite pipe is maleic grafted polyethylene used for PE-AL-PE, PEX-AL-PEX and PERT-AL-PERT composite pipes. Lushan adhesive resin could provides i.. |
|||
Melting Point | 126 °C | 259 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 41E556 Anhydride-Modified LLDPE Adhesive Resin Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Melting Point | 126 °C | 259 °F | ASTM D3417 |
Total CD 4300 HDPE extrusion Applications: General profile extrusion, irradiation-crosslinked productsInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product.. |
|||
Melting Point | 126 °C | 259 °F | ASTM D3417 |
Total HL 428 HDPE film resin Applications: multi-wall liner, poultry multi-layer gas flush bags, mailing envelopes, heavy-duty shipping sacks, fresh cut produce packaging, coextrusionInformation provided provided by Total Petro.. |
|||
Melting Point | 126 °C | 259 °F | ISO 11357 |
Total Lumicene® mPE M 4040 Metallocene Polyethylene, Cast Film Lumicene® mPE M 4040 is a Lumicene® metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 4040 can be processed at high output rates with low extrusion pressure, low neck-in, ex.. |
|||
Melting Point | 126 °C | 259 °F | ISO 11357 |
Total Lumicene® mPE M 4041 UV Metallocene Polyethylene, Rotomolding Lumicene® mPE M 4041 UV is a new generation metallocene medium density polyethylene with hexene as comonomer.Lumicene® mPE M 4041 UV is intended for the manufacture of rotomolded items.Lumicene® .. |
|||
Melting Point | 126 °C | 259 °F | ASTM D3417 |
Total MDPE HL 323 Medium Density Polyethylene, Film Resin Medium molecular weight, medium density film resinCharacteristics:Excellent balance of stiffness and impact strengthGood puncture resistanceExcellent compatibility with LDPE and LLDPEGood tensile st.. |
|||
Melting Point | 126 °C | 259 °F | Dow Method (DSC) |
Dow DNDA-1081 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-1081 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow |
|||
Melting Point | 126 °C | 259 °F | Dow Method (DSC) |
Dow DNDA-9810 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-9810 NT 7 is produced using UNIPOL™ PE process technology and is supplied in pellet form. This resin is specifically designed as a carrier resin for color concentrates and other masterbat.. |
|||
Melting Point | 126 °C | 259 °F | Dow Method (DSC) |
Dow DOWLEX™ 2038.68G Linear Low Density Polyethylene Fast processing on narrow die gaps For blown film paper product over wrap applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Melting Point | 126 °C | 259 °F | Dow Method (DSC) |
Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7065 NT 7 is a fractional melt, ethylene-hexene copolymer, designe.. |
|||
Melting Point | 126 °C | 259 °F | Dow Method (DSC) |
Dow DNDB-1077 NT 7 Linear Low Density Polyethylene Resin DOW DNDB-1077 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow |
|||
Melting Point | 126 °C | 259 °F | Dow Method (DSC) |
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Strength High Output Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7041 NT 7 is a half melt, ethylene-hexene copolymer, designe.. |
|||
Melting Point | 126 °C | 259 °F | Dow Method (DSC) |
Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7094 NT 7 is a fractional melt, ethylene-hexene copolymer, designe.. |
|||
Melting Point | 126 °C | 259 °F | DSC |
Arkema Group OREVAC® 18350 Grafted Maleic Anhydride Polyethylene OREVAC 18350 is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE and HDPE coating for steel pipeline. It is mainly used in pipe coating to have good adhesion per.. |
|||
Melting Point | 126 °C | 259 °F | ASTM-D3418 |
Braskem ML4400N LLDPE Rotomolding Polyethylene The resin ML4400N is a linear low-density polyethylene, 1-butene based, with high stiffness and an adequate balance of processability and environmental stress cracking resistance. It contains long t.. |
|||
Melting Point | 126 °C | 259 °F | ASTM D3418 |
ExxonMobil LL 8555.67 Rotational Molding Resin
(discontinued **) LL 8555 is a linear low density hexene copolymer designed to offer excellent processability, dimensional control, whiteness and low warpage. This resin is ideally suited for applications that requir.. |
|||
Melting Point | 126 - 128 °C | 259 - 262 °F | Average value: 126 °C Grade Count:5 |
Overview of materials for Medium Density Polyethylene (MDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max.. |
|||
Melting Point | 126 °C | 259 °F | ASTM D3417 |
Total CD 471 HDPE conduit Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines. |
|||
Melting Point | 126 °C | 259 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 4107 Anhydride-Modified LLDPE Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |