Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 100 °C | 212 °F | ASTM D3418 |
Petroquimica Triunfo Tritheva® TN 2020 EVA Copolymer The Tritheva TN 2020 resin is a Ethylene-Vinyl Acetate copolymer (EVA) developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Th.. |
|||
Melting Point | 100 - 230 °C | 212 - 446 °F | Average value: 170 °C Grade Count:43 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Melting Point | 100 °C | 212 °F | DSC; ASTM D3418 |
DuPont Bynel® 30E699 Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 100 °C | 212 °F | Freezing Point, DSC; ASTM D3418 |
DuPont Bynel® 41E623 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Melting Point | 100 °C | 212 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 3080 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 100 °C | 212 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3121A Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
(discontinued **) 7.5 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dr.. |
|||
Melting Point | 100 °C | 212 °F | DSC; ASTM D3418 |
DuPont™ Surlyn® 1652SBR Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating
(discontinued **) Surlyn® 1652SBR is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to pro.. |
|||
Melting Point | 100 °C | 212 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5020 400 Micron LDPE Powder Description: ICOFLO 510-5020 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melting Point | 100 °C | 212 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5062 500 Micron LDPE Powder Description: ICOFLO 510-5062 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melting Point | 100 °C | 212 °F | DSC; ASTM D3418 |
ICO Polymers ICOTEXâ„¢ 520-5016 300 Micron LDPE Powder Description: ICOTEX 520-5016 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and a .. |
|||
Melting Point | 100 °C | 212 °F | DSC; ASTM D3418 |
ICO Polymers ICOTEXâ„¢ 520-5050 500 Micron LDPE Powder Description: ICOTEX 520-5050 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and fa.. |
|||
Melting Point | 100 °C | 212 °F | Eutectic |
Indium Corp. Indalloy 41 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 100 - 110 °C | 212 - 230 °F | |
Fine Organics FINALUX GT 23 Composite Lubricant Applications: One pack lubricant specially suggested for RPVC pressure pipes and commercial pipes, suitable for single as well as twin screw extruders.Information provided by Fine Organics |
|||
Melting Point | 100 °C | 212 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5064 1200 Micron LDPE Powder Description: ICOFLO 510-5064 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melting Point | 100 - 130 °C | 212 - 266 °F | |
LG Chemical LUTENE CCO550BK PE Compound Description: LUTENE CC0550BK offer the following properties: high mechanical properties, good environmental stress cracking resistance, excellent wetherability and high speed extrusion to give a smo.. |
|||
Melting Point | 100 - 160 °C | 212 - 320 °F | |
Sibur AGG-G/B Atactic Polypropylene For preparation of polymer, bitumen-polymer and polymer-mineral mastics. Individual melts and compositions used for anti-corrosion covers for underground piping, different building structures, stru.. |
|||
Melting Point | 100 - 160 °C | 212 - 320 °F | |
Sibur APP-G Atactic Polypropylene For preparation of polymer, bitumen-polymer and polymer-mineral mastics. Individual melts and compositions used for anti-corrosion covers for underground piping, different building structures, stru.. |
|||
Melting Point | 100 °C | 212 °F | Freezing Point; ASTM D3418 |
DuPont™ Bynel® 50E739 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Melting Point | 100 °C | 212 °F | DSC; ASTM D3418 |
DuPont™ Surlyn® 1652 Zinc Ionomer Resin for Flexible Packaging Surlyn® 1652 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene .. |
|||
Melting Point | 100 °C | 212 °F | DSC, 10°C/min; DuPont Test |
Dow Engage® 8480 Polyolefin Elastomer Description: Engage® 8480 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in footwear applications and profile extrusion of tubing and hoses. It has good clari.. |
|||
Melting Point | 100 °C | 212 °F | 10°C/min |
Arkema Group Evatane® 1010 VN 3 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible, transparent films with high mechanical properties. Examples: stretch film, food packaging.ISO data provided by t.. |
|||
Melting Point | 100 °C | 212 °F | ASTM D3417- ISO 3146 |
DuPont Elvax® 760Q Ethylene Vinyl Acetate DuPont™ Elvax® 760W is a low BHT anti-oxidant ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications: Elvax® 760Q resins can be used for the following applicati.. |