Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | -2.00 °C | 28.4 °F | TR 10 |
3M Dyneon™ PFE 133TBZ High Temperature Perfluoroelastomer 3M™ Dyneon™ PFE 133TBZ is a technically advanced high temperature perfluorelastomer (HT PFE). It is designed to meet the challenges of higher temperature plasma applications. It is classified as F.. |
|||
Transformation Temperature | -2.00 °C | 28.4 °F | TR10 |
3M Dyneon™ 131TZ High Temperature Perfluoroelastomer 3M™ Dyneon™ 131TZ is a technically advanced high temperature perfluoroelastomer (HT PFE). It is designed to meet the challenges of higher temperature applications. It is classified as FFKM per AST.. |
|||
Transformation Temperature | -2.00 °C | 28.4 °F | TR10 |
3M Dyneon™ 81TZ High Temperature Perfluoroelastomer 3M™ Dyneon™ PFE 81TZ is a technically advanced high temperature perfluoroelastomer (HT PFE). It is designed to meet the challenges of higher temperature applications. It is classified as FFKM per .. |
|||
Transformation Temperature | -2.00 °C | 28.4 °F | TR10 |
3M Dyneon™ PFE 4131TZ High Temperature Perfluoroelastomer 3M™ Dyneon™ PFE 4131TZ is an incorporated cure high temperature perfluoroelastomer (HT PFE). It is designed to meet the challenges of higher temperature applications. It is classified as FFKM per .. |
|||
Transformation Temperature | -2.00 °C | 28.4 °F | TR10 |
3M Dyneon™ PFE 60Z Perfluoroelastomer Dyneon™ PFE 60 Z is a technically advanced peroxide curable perfluoroelastomer, designed to meet the challenges of demanding sealing applications. It’s fully fluorinated back bone structure provid.. |
|||
Transformation Temperature | -2.00 °C | 28.4 °F | TR10 |
3M Dyneon™ PFE 80Z Peroxide Cure Perfluoroelastomer 3M™ Dyneon™ Peroxide Cure Perfluoroelastomer PFE 80Z is a technically advanced peroxide curable perfluoroelastomer. This product is designed to have improved acid resistance and lower metal ion ex.. |
|||
Transformation Temperature | -2.00 °C | 28.4 °F | TR10 |
3M Dyneon™ TFE 90Z Peroxide Cure Perfluoroelastomer 3M™ Dyneon™ Peroxide Cure Perfluoroelastomer PFE 90Z is a technically advanced peroxide curable perfluoroelastomer, designed to meet the challenges of demanding sealing applications. It is classif.. |
|||
Transformation Temperature | -2.00 °C | 28.4 °F | TR 10 |
3M Dyneon™ PFE 132TBZ High Temperature Perfluoroelastomer 3M™ Dyneon™ PFE 132TBZ is a technically advanced high temperature perfluorelastomer (HT PFE). It is designed to meet the challenges of higher temperature plasma applications. It is classified as F.. |
|||
Transformation Temperature | -2.00 °C | 28.4 °F | TR 10 |
3M Dyneon™ PFE 191TZ High Temperature Perfluoroelastomer 3M™ Dyneon™ PFE 81TZ, PFE 131TZ and PFE 191TZ are technically advanced high temperature perfluorelastomers (HT PFE). They are designed to meet the challenges of higher temperature applications. Th.. |