Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 0.800 µm/m-°C

@Temperature 20.0 °C
0.444 µin/in-°F

@Temperature 68.0 °F
Ineos ABS Lustran® H604
Standard impact strength.,Property data per ISO test methods.
CTE, linear, Parallel to Flow 0.800 µm/m-°C

@Temperature 20.0 °C
0.444 µin/in-°F

@Temperature 68.0 °F
Ineos ABS Lustran® H606 LS
Improved heat and UV resistance.,Property data per ISO test methods.
CTE, linear, Parallel to Flow 0.800 µm/m-°C

@Temperature 20.0 °C
0.444 µin/in-°F

@Temperature 68.0 °F
Ineos ABS Lustran® H607AS
Contains antistatic additives,Property data per ISO test methods.
CTE, linear, Parallel to Flow 0.800 µm/m-°C

@Temperature 20.0 °C
0.444 µin/in-°F

@Temperature 68.0 °F
Ineos ABS Lustran® H702
Medium heat resistance, increased flow. ,Property data per ISO test methods.
CTE, linear, Parallel to Flow 0.800 µm/m-°C

@Temperature 20.0 °C
0.444 µin/in-°F

@Temperature 68.0 °F
Ineos ABS Lustran® H801
High heat resistance, PC modified, low emission, increased flow.,Property data per ISO test methods.
CTE, linear, Parallel to Flow 0.800 µm/m-°C

@Temperature 20.0 °C
0.444 µin/in-°F

@Temperature 68.0 °F
Ineos ABS Lustran® H802
High heat resistance, increased flow.,Property data per ISO test methods.
CTE, linear, Parallel to Flow 0.800 µm/m-°C

@Temperature 20.0 °C
0.444 µin/in-°F

@Temperature 68.0 °F
Ineos ABS Lustran® M201AS
Increased chemical resistance compared to P2x, contains antistatic additives.,Property data per ISO test methods.