Polymer Property : CTE, linear, Parallel to Flow = 16.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 13.0 - 16.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
7.22 - 8.89 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
BASF Ultradur B 4500 PBT
Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660.
CTE, linear, Parallel to Flow 14.0 - 16.0 µm/m-°C

@Temperature 50.0 - 150 °C
7.78 - 8.89 µin/in-°F

@Temperature 122 - 302 °F
ISO 11359-2
Raschig Group DECAL® 152CL Phenolic
Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet..
CTE, linear, Parallel to Flow 13.0 - 16.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
7.22 - 8.89 µin/in-°F

@Temperature 73.4 - 176 °F
BASF Ultradur B 4520 PBT
Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade.
CTE, linear, Parallel to Flow 13.0 - 16.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
7.22 - 8.89 µin/in-°F

@Temperature 73.4 - 176 °F
BASF Ultradur B 6550 PBT
Ultradur B 6550 is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes.