Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 65.0 - 100 µm/m-°C | 36.1 - 55.6 µin/in-°F | ASTM D696 |
LG Chemical LUMID HI5063A(W) PA6/ABS+MF6%, High Impact Feature: Injection Molding, PA6/ABS+MF6%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
CTE, linear, Parallel to Flow | 70.0 - 100 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 55.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3L PA6 (Dry) Ultramid B3L is an impact-modified, easy flowing injection molding PA6 grade for fast processing. |
|||
CTE, linear, Parallel to Flow | 70.0 - 100 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 55.6 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® A4H PA66 (Dry) Description: Highly heat aging resistant, medium-viscosity injection-molding grade for highly stressed parts such as bearing cages, gearwheels, spool bodies and chain drive tensioners.Information pr.. |
|||
CTE, linear, Parallel to Flow | 70.0 - 100 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 55.6 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3K BK00464 PA6 (Dry) Description: Easy flowing and stabilized injection-molding grade used for technical parts with wall thicknesses >2 mm, e.g. machinery components, fans and power tool housings.Information provided by.. |
|||
CTE, linear, Parallel to Flow | 70.0 - 100 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 55.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3K PA6 (Dry) Ultramid B 3K is an easy flowing, stabilized for fast processing, grade of nylon 6. |
|||
CTE, linear, Parallel to Flow | 70.0 - 100 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 55.6 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3L BK00464 PA6 (Dry) Description: Impact-modified, free-flowing and rapidly processable injection-molding grade for dry impact-resistant technical articles such as, for example, housings, fittings, small parts and wall .. |
|||
CTE, linear, Parallel to Flow | 60.0 - 100 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 55.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® C3U PA66/6 (Dry) Ultramid C3U is an injection molding, general purpose PA66/6 grade with improved flame retardance. |
|||
CTE, linear, Parallel to Flow | 70.0 - 100 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 55.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3S BK00464 PA6 (Dry) Ultramid B3S BK00464 is an easy flowing, pigmented black, finely crystalline injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
CTE, linear, Parallel to Flow | 70.0 - 100 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 55.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3S HP PA6 (Dry) Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing |