Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | Recommended |
Nye Lubricants 350-SBG-2 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | Recommended |
Nye Lubricants UniFlor 8622 (851) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | Recommended |
Nye Lubricants UniFlor 8622R (851RP) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | Temperature at which stiffness does not exceed 70 Mpa |
Precision Polymer Engineering N80N Nitrile Rubber Nitrile Rubber, 76-85 °IRHD. Copolymer of acrylonitrile and butadiene. Meets Aerospace Specification DTD5595A Grade 80. ASTM designation = NBR. ISO designation = NBR.Applications: Sealing petroleum.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | T10 |
Precision Polymer Engineering P90B Polyacrylate Rubber Polyacrylic or Polyacrylate Rubber, 85-95 °IRHD. Copolymer of ethyl acrylate and vinyl ether. ASTM & ISO designation = ACM.Applications: Extensively used in automotive transmission systems. Superi.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G50S FFKM White Perfluoroelastomer Perlast® G50S FFKM is a White Perfluoroelastomer 50-55 °IRHD. It has excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and extr.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G60A Perfluoroelastomer A black general purpose perfluoroelastomer compound with excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Suitable for app.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G60H Perfluoroelastomer Special, pure white compound with excellent high temperature properties and wide chemical resistance. Extremely low outgassing properties.Applications: For use in applications which require exposur.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G60S FFKM White Perfluoroelastomer Perlast ® G60S FFKM is a White Perfluoroelastomer 56-65 °IRHD. It has excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and ext.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G60T Perfluoroelastomer A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: This grade is particularly suited to static ap.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G67P Translucent Perfluoroelastomer A translucent beige compound with semi-crystalline perfluoropolymer nano-filler, specially developed to meet the demands of the semiconductor and bio-analytical industries. Compatible with fluorine .. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G70T Perfluoroelastomer A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require long-ter.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G80H Perfluoroelastomer Special, pure white compound with high temperature properties and wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing p.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G80T Perfluoroelastomer A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require long-ter.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G90S White Perfluoroelastomer Perlast ® G90S is a White Perfluoroelastomer 86-95 °IRHD with excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and formulated .. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G92A Perfluoroelastomer An electrically conductive black perfluoroelastomer with excellent chemical and steam resistance.Applications: Specially formulated for applications requiring special electrical properties. Origina.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering V75K Fluoroelastomer Compound Fluoroelastomer Rubber, 70-80 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out: MHK710, A1-10, B37, B38, EF31, EO78, Z1. Wher.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering V85C Fluoroelastomer Compound Green Fluoroelastomer Rubber, 80-90 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out:- MHK710, A1-10, B38, EF31, EO78, Z1, Z2,.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering V85K Fluoroelastomer Compound Fluoroelastomer Rubber, 80-90 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out M3HK910, A1-10, B37, B38, EF31, EO78, Z1. Wher.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G71H Perfluoroelastomer Special, white compound, with PTFE blended for improved dynamic performance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties. Appl.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G75B High Temperature Perfluoroelastomer Perlast® G75B offers a unique blend of excellent chemical resistance, temperature capabilities and mechanical properties, simultaneously extending the operating limits in all three aspects. Perlas.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G75S Perfluoroelastomer Perlast® G75S has been specifically developed to cope with a wide range of process media, potent active pharmaceutical ingredients (APIs) and aggressive cleaning agents, being especially suited to .. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering V60L Fluoroelastomer Compound Special steam resistant, Fluoroelastomer Rubber, 55-65 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out: M2HK610, A1-10, B37, B38, EF31, EO78, F15.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Manifattura Cattaneo PVC U Polyvinyl Chloride Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Freudenberg Simrit Simriz® 484 FDA FFKT Perfluoroelastomer Compound Perfluoro elastomers – or FFKM for short – have an ideal combination of characteristics, with their excellent chemical resistance, high level of temperature resistance, and high levels of .. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Trelleborg B700 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Trelleborg B800 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
ChevronTexaco NLGI 1 Ultra Duty Grease EP FeaturesChevron Ultra-Duty Greases EP are versatile, multipurpose extreme pressure greases with high adhesive propertues designed for a wide variety of automotive and industrial applications.They ar.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | Application |
3M 7142 Repositionable Paper Label Material 3M™ Repositionable Paper Label Material 7113 and 7142 with 3M™ Adhesive 1000 offer unique, one-piece removability from many surfaces, including fragile papers, and can be repositioned repeatedly f.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | Approx. Cold test |
Lubriplate 176 No. Inorganic/Organic Grease For Open Gearing This adhesive, semi-fluid grease is used for all types of open gears lubricated by centralized systems. Provides good pumpability without the use of harmful solvents. Applications: Open gears lubric.. |