Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -110 °C | -166 °F | |
Aptek 2710A/B Low modulus silicone adhesive Low modulus silicone adhesive; -110ºC to 260ºC operating range; Low outgassing/space grade; Electrostatically Discharging (ESD)APTEK 2710-A/B is a two component, black, low modulus, thixotropic, s.. |
|||
Minimum Service Temperature, Air | -110 °C | -166 °F | |
Aptek 2712-A/B Very low stress silicone adhesive Very low stress silicone adhesive; -110ºC to 260ºC operating range; Low outgassing/space gradeAPTEK 2712-A/B is a two component, white, very soft, thixotropic, electrically insulative, silicone ad.. |