Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 50.0 °C | 122 °F | Application |
3M 7000 Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Minimum Service Temperature, Air | 50.0 °C | 122 °F | Application |
3M 7000FL Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Minimum Service Temperature, Air | 50.0 °C | 122 °F | Application |
3M 7000FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Minimum Service Temperature, Air | 50.0 °C | 122 °F | Application |
3M 7002 Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Minimum Service Temperature, Air | 50.0 °C | 122 °F | Application |
3M 7002FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Minimum Service Temperature, Air | 50.0 °C | 122 °F | Application |
3M 7014 Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Minimum Service Temperature, Air | 50.0 °C | 122 °F | Application |
3M 7014FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Minimum Service Temperature, Air | 50.0 °C | 122 °F | Application |
3M 7026 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Minimum Service Temperature, Air | 50.0 °C | 122 °F | Application |
3M 7042 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Minimum Service Temperature, Air | 50.0 °C | 122 °F | Application |
3M 7011 Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Minimum Service Temperature, Air | 50.0 °C | 122 °F | Application |
3M 7011FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Minimum Service Temperature, Air | 50.0 °C | 122 °F | Application |
3M 7014FL Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Minimum Service Temperature, Air | 50.0 °C | 122 °F | Application |
3M 7028 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Minimum Service Temperature, Air | 50.0 °C | 122 °F | Application |
3M 7028FL Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Minimum Service Temperature, Air | 50.0 °C | 122 °F | Application |
3M 7031 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Minimum Service Temperature, Air | 50.0 °C | 122 °F | Application |
3M 7033 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Minimum Service Temperature, Air | 50.0 °C | 122 °F | Application |
3M 7035 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Minimum Service Temperature, Air | 50.0 °C | 122 °F | Service |
3M 7037 Screen Printable Polyester Performance Label Product 3M™ Screen Printable Polyester Performance Abel Product 7037 is a durable, high performance material that offers excellent thermal stability and moisture resistance. This polyester label stock util.. |
|||
Minimum Service Temperature, Air | 50.0 °C | 122 °F | Application |
3M 7911FL Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Minimum Service Temperature, Air | 50.0 °C | 122 °F | |
3M 853 Polyester Tape 3M™ Polyester Tape 853 is comprised of strong, thin polyester backing with high shear, solvent resistant acrylic adhesive. These qualities make this tape ideal for applications where solvent exposu.. |