Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Recommended |
Nye Lubricants FTL-9000 Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Lower limit of working range |
Heatbath/Park #50 Oil Quench Low viscosity quench oil that approaches water in quench speed, yet gives a more uniform, less severe quench than water. Recommended for open quench system operating below 120°C.Information provi.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ 1000-41 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ 1000LF-114 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Application |
3M ScotchCal™ 3690E Graphic Film Material 3M™ ScotchCal™ Graphic Film Materials 3690E and 3698E are flexible cast vinyl films suitable for conforming to curved and textured surfaces, including most low surface energy plastics and small di.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7125-103 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7125-15 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7125-59 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7125-66 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7725-15 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7725-90 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ IJ3650-10 Graphic Film 2-mil, opaque white and transparent film; Pressure-sensitive adhesive; Permanent filmInformation provided by 3M |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Air and substrates, for flat surfaces without rivets |
3M Scotchlite™ 5100 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Pressure-sensitive adhesive; Permanent; Available in 15 colors, including black (which reflects whit.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | flat surfaces without rivets |
3M Scotchlite™ 680-71 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | flat surfaces without rivets |
3M Scotchlite™ 680-72 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Air and substrates, for flat surfaces without rivets |
3M Scotchlite™ RG5100R-10 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Pressure-sensitive adhesive; Removable with heat; Available in 15 colors, including black (which ref.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Application |
3M 7000PL Photoluminescent Film 3M Photoluminscent Film 7000PL is a high performance photoluminescent for film for safety and emergency exit signage. Meets and exceeds ASTM E207210, IMO A.752, OSHA 1910, 2000 IBC, DIN-67510 Part 4.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Application |
3M 7604FP Primalyn™ White Vinyl Label Material 3M™ Primalyn™ White Vinyl Label Material 7604FP is a flexible vinyl providing excellent squeeze bottle performance with consistent printability. This material utilizes 3M™ Adhesive 300, which has.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Curved or corrugated surfaces with rivets |
3M Controltac™ 180C Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Application |
3M FP02450N Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3800, which is an ultra removable acrylic designed t.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7125-31 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7125-53 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7725-177 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7725-357 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7725-88 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | flat surfaces without rivets |
3M Scotchlite™ 680-76 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Application |
3M 7776 Polypropylene Label Material 3M™ Polypropylene Label Material 7776 is a durable polypropylene label stock that offers excellent performance in applications requiring surface conformability. This label product utilizes 3M™ Adh.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Curved or corrugated surfaces with rivets |
3M Controltac™ 180 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Curved or corrugated surfaces with rivets |
3M Controltac™ 8620C ES Changeable Graphic Film with Comply™ Adhesive These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7725-57 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |