Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
Nye Lubricants 309 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
Nye Lubricants 5301 (SVLG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
Nye Lubricants 572H-10 Dispersion Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
Nye Lubricants 704C (IG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
Nye Lubricants 750A (IG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
Nye Lubricants UniFlor 8921SU (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
Nye Lubricants UniFlor 8921 (892-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Precision Polymer Engineering F80R Fluorosilicone Rubber Red Fluorosilicone, 76-85 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification DTD5583A Grade 80.Applications: |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Precision Polymer Engineering S50N Silicone Rubber Silicone Rubber, 45-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ. To meet UK Ministry of Defence Aircraft Materials .. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
NextGen Adhesives G907-27 Structural Adhesive Description: NGAC G907-27 is a medium viscosity polyamide adhesive system utilized extensively in industrial and structural applications.Advantages and Applications: The NGAC G907-27 provides excell.. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Resin Technology Group 350 Surface Insensitive Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 350 Surface Insensitive Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Resin Technology Group 395 Plastics, Large Gap Fill Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 395 Plastics, Large Gap Fill Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Brittleness Temperature |
DuPont Performance Polymers Hypalon® 45 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound
(d Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato.. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Resinlab® RC8038 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Resinlab® RC8041 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Resinlab® RC8060 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Humiseal 1A27 Urethane Conformal Coating Humiseal 1A27 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedPasses thermal shock test (MIL-I-46058C)Flammabilit.. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Humiseal 1B73LSE Acrylic Conformal Coating Humiseal 1B73LSE Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityUL Approval PendingMIL-I-46058C Approval Pendin.. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Humiseal 1C65 Silicone Conformal Coating Humiseal 1C65 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Fujipoly Industries Zebra® LT 200 Low Temperature Carbon Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Trelleborg Emerson & Cuming Eccobond® 24 LV General Purpose Catalyst Emerson & Cuming 24 LV Eccobond® General Purpose CatalystFaster curing, shorter working life version of 23 LV. Recommended for small mass castings due to higher exotherm. Cure Type: Room Temp or He.. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Trelleborg Emerson & Cuming Stycast® 5952 Two-Component Easy Mix Ratio Encapsulant Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, .. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Trelleborg Emerson & Cuming Stycast® E 1400 Two-Component General Purpose Encapsulant Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as .. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Aremco Aremco-Bond™ 568 High Performance Epoxide Aluminum-Filled, 1:1, Good Bond Strength and High Thermal Conductivity. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
Nye Lubricants 5300 (SVLG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
Nye Lubricants 761 (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Parker Chomerics CHO-SHIELD® 2002 Conductive Coating Electrically conductive coatings provide corrosion protection for enclosure flanges which mate with EMI shielding gaskets. They can also provide a corrosion resistant conductive surface coating on a.. |
|||
Minimum Service Temperature, Air | -65.0 - -27.0 °C | -85.0 - -16.6 °F | Average value: -41.9 °C Grade Count:17 |
Overview of materials for PVC, Wire and Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr.. |
|||
Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
Resinlab® RC8035 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |