Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 5163X0085 0.0085" (0.216 mm) Cured Silicone Rubber with Fiberglass Substrate
(discontinued **) 50 inches Overall Width. Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone RubberProduct Description: Acoustical dampeningAppearance: Silver silicone on fiberglass clothThis d.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 10842S020 0.020" (0.508 mm) Fully Cured, Unsupported, Silicone Rubber Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber Appearance: Dark red silicone rubberThis data represents typical values for the production material. The data should not be used.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 10842S060 0.060" (1.52 mm) Fully Cured, Unsupported, Silicone Rubber Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber Appearance: Dark red silicone rubberThis data represents typical values for the production material. The data should not be used.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 41580R015 0.015" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 49581R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 51141R015 Silicone Rubber/Fiberglass Laminate Interleave 1: 3 mil PE; Side 1: uncured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave 2: 3 mil PE |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 55629R028 0.0285" (0.724 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Appearance: Red silicone gum on fiberglassThis data repre.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 55869R062 0.062" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 56141R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass Side 1: Uncured Silicone Rubber This data represents typical values for the production m.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 56976B026 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon P29514R020 0.0205" (0.521 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassAppearance: Red silicone rubber on fiberglass fabric.This data represents typical values for the product.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon R33920W028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance: White gum on glass fiber fabricThis data Represents typical values for the production material. The data should not be used to write, .. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon R35066R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon R37292S018 0.018" (0.457 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberCarrier: PTFE Coated FiberglassThis data represents typical values for the production material. The data should not be used .. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 30860R060 0.60" Uncured Silicone Rubber on a Kodacel Carrier Design/Construction:Interleave: 0.003" Low Density PolyethyleneAdd-on: Uncured Silicone RubberSubstrate: Kodacel CarrierThis data represents typical values for the production material and should .. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 44571XB015 0.015" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass (Flexible Heater Substrate) Side 2: Uncured Silicone RubberInterleave: 2.5 mil .. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 51344R020 0.020" (0.508 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Semi-Cured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 51581R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 55106R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 55146XA028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber This data represents typical values for the production mat.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 55149R028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red si.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 55276B028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Cured Silicone Rubber This data represents typical values for the production mate.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 55638R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 55949C028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber Appearance: Brown silicone rubber and gum on fiberglass clothThis data Represents typical values for the produc.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon R35928R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: .. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon T3020-B002-## 0.020" Self-Fusing, Cured Silicone Rubber Tape with Fiberglass Substrate 0.5 inch wide, 20 mil thick, black, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the ## characters in the part number... |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 32980X078 0.078" Uncured Silicone Rubber on Polyester Film Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as ma.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 44141R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Clear PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Blue PolyethyleneThis data represent.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 44568R016 0.016" (0.406 mm) Cured/Uncured Layers Uncured Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, mat.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon R37879X034 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: Cured silicone rubber; Substrate: 162 fiberglass |