Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Protective Coating PC-11® White Epoxy Paste PC-11® is a Heavy Duty-white epoxy Paste formulated by the manufacturer of PC-7.® After mixing, PC-11® can be applied to a dry, wet or underwater surface and will cure to an off white color. PC.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Alcoa KAMA 3300 Very High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coat.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 2102 C.I. SBR/NBR Sheet Rubber, Polyester Insert Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2102 C.I. is a smooth.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 2103 C.I. SBR/NBR Sheet Rubber, Polyester Insert Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2103 C.I. is a smooth.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 362 Nitrile Sheet Rubber Nitrile sheet is primarily used for applications where resistance to oil, solvents and fuels is required.Style #362 is a white nitrile sheet made from FDA-approved ingredients per Z1 CFR 177.2600. I.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 567 EPDM Sheet Rubber Excellent general purpose gasket materials for air, hot and cold water, saturated steam and exterior service.Black, smooth finish, commercial qualityInformation provided by Garlock Rubber Technologi.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 60 SBR Sheet Rubber SBR rubber specially compounded to be quick-sealing, non-hardening and heat resistant.Red, cloth finish, drum curedInformation provided by Garlock Rubber Technologies |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 7164 SBR Rubber Lining SBR rubber lining for protection applications such as chute lining and skirtboards.An optional duck fabric backing is available.Information provided by Garlock Rubber Technologies |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock SBR Extruded Skirtboard SBR rubber extruded skirtboard for protection applicationsInformation provided by Garlock Rubber Technologies |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock Super Rinohideâ„¢ 7160 SBR Rubber Lining SBR rubber lining for protection applications such as chute lining and skirtboards.Super RINOHIDEâ„¢, in particular, performs with superior resistance to abrasion, impact, aging and weathering. .. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Greene Tweed CHEMRAZ® 528 Perfluoroelastomer Chemraz® 528 works well in a wide variety of biotechnology and medical device applications where ling-term seal reliability is required. This seal material offers excellent performance in static.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Greene Tweed FLUORAZ® 888 Fluoroelastomer, FEPM Fluoraz® 888 polytetrafluoroethylene/propylene (FEPM) performs well in aggressive chemicals where ultra pure materials are not required. Recommended for conventional wet and dry system applicatio.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® 2829-3(R) Acrylic Adhesive Zone Tape Specification Notes: 21CFR177.1550 compliant. All data based on a 0.003 inch test sample. Information provided by Saint Gobain Performance Products. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® 2829-5(R) Acrylic Adhesive Zone Tape Specification Notes: UL Guide OANZ2, File E51201, MIL-T-47012, UL510. All data based on a 0.0047 inch test sample.Information provided by Saint Gobain Performance Products. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® G569 Glass Cloth Backing Acrylic Adhesive Pressure Sensitive Tape Description: Glass cloth offers excellent abrasion resistance and mechanical properties, as well as high tensile strength and extreme temperature resistance. Service temperatures range from -100°.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® M69 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low water absorptio.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® M705 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® M765 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® M97 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain Tygon® LP 1600 Low Permeation Fuel Tubing Tygon® LP1600 Low Permeation Fuel Tubing is designed to meet new marine market emission standards. Applications Marine boats with above-deck outboard engines Personal watercraft -- Jet Skis, .. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® K109 Polyimide Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain Tygon® LP 1100 Low Permeation Fuel Tubing Tygon® LP1100 Low Permeation Fuel Tubing is designed to meet new emission standards. Applications Lawn and garden power equipment Lubricating oil and grease transfer lines Small engine fuel.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Bostik 2385 General Purpose EVA Glue Stick Bostik 2385 General Purpose EVA Glue StickGood general purpose bonding of paper, wood, cardboard, foam and fabrics. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Bostik 110 Low cost EVA Glue Stick Bostik 110 Low cost EVA Glue StickLow cost for porous surfaces. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Bostik 2107 General Purpose EVA Glue Stick Bostik 2107 General Purpose EVA Glue StickGeneral purpose for porous substrates. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Bostik 2305 Good Heat Resistance EVA Glue Stick Bostik 2305 Good Heat Resistance EVA Glue StickGood heat resistance. Adheres to a variety of coated and uncoated board stock. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain Furon®, Kapton® K275 Tape Description: A 1 mil thermally conductive Kapton® film, coated on both sides with 2 mils of thermally-conductive pressure-sensitive adhesive. Recommended uses: Excellent for use in small, compact e.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | Approx. Cold test |
Lubriplate Temp G.S. Low Lithium Based Grease For Open Gearing Lithium-based open gear grease made for all types of open gears. Available in 4 formulas for a variety of conditions and temperatures. Applications: Open gears, slides, fifth wheels, low temps. Gear.. |