Polymer Property : Vicat Softening Point = 237 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 114 °C
237 °F
10 N - 120°C/h; ISO 306/A120
Polimeri Europa Sinkral® C 442 ABS Resin
Sinkral C 442 is a heat resistant injection molding grade offering good flow and impact resistance together with excellent thermal stability during processing. Designation: Thermoplastic ISO 2580-AB..
Vicat Softening Point 114 °C
237 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
Vicat Softening Point 114 °C
237 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties
Vicat Softening Point 114 °C
237 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East)
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by..
Vicat Softening Point 114 °C
237 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS
Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.
Vicat Softening Point 114 °C
237 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Lexan® BPL1000 PC (Asia Pacific)
Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U..
Vicat Softening Point 114 °C
237 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Lexan® BPL1000 PC (Europe-Africa-Middle East)
Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U..
Vicat Softening Point 114 °C
237 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific)
Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior ..
Vicat Softening Point 114 °C
237 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific)
Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior ..
Vicat Softening Point 114 °C
237 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Lexan® ML7677 PC (Asia Pacific)
Transparent Polycarbonate in limited colors. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm
Vicat Softening Point 114 °C
237 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Lexan® ML7677 PC (Asia Pacific)
Transparent Polycarbonate in limited colors. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm
Vicat Softening Point 114 °C
237 °F
ASTM D1525
SABIC R50035 Linear Low Density Polyethylene for Rotational Molding
Product Description: R50035 are Linear Low Density Polyethylene grades designed to provide excellent stress crack resistance, mechanical properties with high rigidity, toughness, gloss and low warp..
Vicat Softening Point 114 °C
237 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East)
Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior ..
Vicat Softening Point 114 °C
237 °F
ISO 306
Total Lacqtene® 2006 PBK 35 HDPE pipe, sheet  (discontinued **)
LACQTENE® 2006 PBK 35 is a medium density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2006 PBK 35 may be used for pipe extrusion (micro-irriga..
Vicat Softening Point 114 °C
237 °F
ASTM D1525
NOVA Chemicals Sclair® 8405 BK, 8405GBK MDPE Rotational Molding Resin  (discontinued **)
Features: Good ESCR, high impact strength.Applications: Spray tanks.Data provided by the manufacturer.
Vicat Softening Point 114 °C
237 °F
ASTM D1525
NOVA Chemicals Sclair® 8405 UV8D, 8405G UV8D MDPE Rotational Molding Resin  (discontinued **)
Features: Good ESCR, high impact strength.Applications: Spray tanks.Data provided by the manufacturer.
Vicat Softening Point 114 °C
237 °F
ASTM D1525
NOVA Chemicals Sclair® 2515 MDPE Injection Molding Resin  (discontinued **)
Features: Excellent processability for applications requiring moderate stiffness and improved toughnessExcellent cold temperature impact properties Applications: Ice cream containersHousewares Deep..
Vicat Softening Point 114 °C
237 °F
ASTM D1525
Micropol Microlin ML27 Linear Polyethylene Rotational Molding Powder
Information provided by Micropol Limited
Vicat Softening Point 114 °C

@Load 5.00 kg
237 °F

@Load 11.0 lb
50°C/h; ASTM D1525
LG Chemical XR407E ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Frame, DVD inner part etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by..
Vicat Softening Point 114 °C
237 °F
B/120; ISO R306
Samsung Cheil Industries Infino® NH-1037 PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Vicat Softening Point 114 °C
237 °F
(50 °C/h / 50N) - B/50; ISO 306
Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Dry)
Terblend N NG-04 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, low mold shrinkage and high heat resistance.Information provided by STYROLUTION, which is a joint ven..
Vicat Softening Point 114 °C
237 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Noryl NH3060 PPE+HIPS
NH3060 resin is a modified PPE + PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific ..
Vicat Softening Point 114 °C
237 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL WCV072 PPE+PP
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
Vicat Softening Point 114 °C
237 °F
10 N; ISO 306A
Borealis Borseal™ TD215BF Terpolymer for BOPP Film
Borseal TD215BF is a C2/C4 terapolymer film resin.Borseal TD215BF is especially developed for use as sealing layers in coextruded BOPP film (manufactured on Stenter frame and double bubble film proc..
Vicat Softening Point 114 °C
237 °F
10 N; ISO 306A
Borealis Borseal™ TD218BF Terpolymer for BOPP Film
Borseal TD218BF is a C2/C4 terapolymer film resin.Borseal TD218BF is especially developed for use as sealing layers in coextruded BOPP film (manufactured on Stenter frame and double bubble film proc..
Vicat Softening Point 114 °C
237 °F
10 N; ISO 306A
Borealis Borseal™ TD211BF Terpolymer for BOPP Film
Borseal TD211BF is a C2/C4 terapolymer film resin especially developed for use as sealing layers in coextruded BOPP film (manufactured on stenter frame and double bubble film process).Borseal TD211B..
Vicat Softening Point 114 °C
237 °F
ASTM D1525
Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7094 NT 7 is a fractional melt, ethylene-hexene copolymer, designe..
Vicat Softening Point 114 - 127 °C
237 - 261 °F
Average value: 119 °C Grade Count:4
Overview of materials for Medium Density Polyethylene (MDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max..
Vicat Softening Point 114 °C
237 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Asia Pacific)
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties
Vicat Softening Point 114 °C
237 °F
Rate B/120; ISO 306
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East)
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..