Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 69.0 - 71.0 °C @Load 5.00 kg |
156 - 160 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RI 50 Rigid PVC, Injection Molding Technical items |
|||
Vicat Softening Point | 69.0 °C @Load 1.02 kg |
156 °F @Load 2.25 lb |
120°C/h, injection molded; ASTM D1525 |
Huntsman IROGRAN® A 85 P 4394 UV TPU-Polyether Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS.. |
|||
Vicat Softening Point | 69.0 °C | 156 °F | ISO 306B |
Lucite International Elvakon® 4494 Low Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Vicat Softening Point | 69.0 °C | 156 °F | ASTM D1525 |
DuPont Elvax® 3150 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 15 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Vicat Softening Point | 69.0 °C | 156 °F | ASTM D1525 |
DuPont Elvax® 3165 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 18 wt% Vinyl Acetate.Elvax® 3165 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Vicat Softening Point | 69.0 °C | 156 °F | ASTM D1525, ISO 306 |
DuPont Elvax® 3165LG Ethylene Vinyl Acetate DuPont™ Elvax® 3165XZ is an extrudable ethylene-vinyl acetate copolymer resin containing low gel material available in pellet form for use in conventional extrusion equipment designed to process p.. |
|||
Vicat Softening Point | 69.0 °C | 156 °F | ASTM-D1525 |
Westlake EF532 12% EVA Copolymer (Experimental Product) Westlake EF532 resin is a 12.0% EVA copolymer designed for use as a sealant / lamination layer in monolayer or coextruded flexible film structures. It has very low seal initiation temperature, excel.. |
|||
Vicat Softening Point | 69.0 °C | 156 °F | ASTM D1525 |
Westlake Elevate™ DA532 Ethylene Vinyl Acetate Copolymer Experimental ProductDescription: Westlake DA532 resin is a 12.0% EVA copolymer designed for use as a sealant / lamination layer in monolayer or coextruded flexible film structures. It has very low .. |
|||
Vicat Softening Point | 69.0 °C | 156 °F | A<sub>50</sub> (10N); ASTM D1525 - ISO 306 |
DuPont Elvaloy® 2112 AC Ethylene and 12% Ethyl Acrylate Copolymer Elvaloy® 2112 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for tubing is various applications. The.. |
|||
Vicat Softening Point | 69.0 °C | 156 °F | ISO 306 |
Total EVA 1005 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 5 is made by a high pressure tubular process. Grade for films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: Coextrusion, stretch .. |
|||
Vicat Softening Point | 69.0 °C | 156 °F | ASTM D1525 |
Eastman Embrace LV Copolyester for Extruded/Cast Film Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo.. |
|||
Vicat Softening Point | 69.0 °C | 156 °F | ASTM D1525 |
Eastman Embrace LV Copolyester for Shrink Film Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo.. |
|||
Vicat Softening Point | 69.0 °C | 156 °F | ASTM D1525 |
Chevron Phillips K-Resin® XK41 Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene CopolymerCustomer Benefits: XK41 is an extrusion grade of K-Resin SB copolymer designed specifically for improved performance in blends with general purpose polystyrene. It is eas.. |
|||
Vicat Softening Point | 68.9 °C | 156 °F | 50°C/hr; 10N; ASTM D1525 |
Arkema Group Solarkote® P-610 Acrylic PVC Capstock, clear, low glossInformation provided by Arkema Group |
|||
Vicat Softening Point | 69.0 °C @Load 0.999 kg |
156 °F @Load 2.20 lb |
ASTM D1525 |
Arkema Group LOTADER® 4210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 4210 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 4210 is a versatile adhesive for extrusion coating or lam.. |
|||
Vicat Softening Point | 68.9 °C | 156 °F | 50°C/hr; 10N; ASTM D1525 |
Arkema Group Solarkote® P-600 Acrylic PVC Capstock, clear, high glossInformation provided by Arkema Group |
|||
Vicat Softening Point | 68.9 °C | 156 °F | 50°C/hr; 10N; ASTM D1525 |
Arkema Group Solarkote® P-601 Acrylic PVC Capstock, white, high glossInformation provided by Arkema Group |
|||
Vicat Softening Point | 68.9 °C | 156 °F | 50°C/hr; 10N; ASTM D1525 |
Arkema Group Solarkote® P-611 Acrylic PVC capstock, white, low glossInformation provided by Arkema Group |
|||
Vicat Softening Point | 69.0 °C | 156 °F | ASTM D1525 |
Chevron Phillips K-Resin® BK18 Styrene-Butadiene Copolymer
(discontinued **) Characteristics: Good flexibilityGood impact resistanceGood clarityGood mold releaseApplications: ToysOvercapsConsumer productsInformation provided by Chevron Phillips. |
|||
Vicat Softening Point | 69.0 °C | 156 °F | Rate B; ASTM D-1525 |
ExxonMobil Iotek® 7310 Zinc Ionomer
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low melt index zinc ionomer made from an ethylene acrylic acid base polymer.Applications: Injection molding; Impact modifier of polyamide. |