Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 52.0 °C | 126 °F | 50°C/h 50N; ISO 306 |
LATI LATISTAT 43/7-02 Low Density Polyethylene (LDPE) Base Conductive Plastic
(discontinued **) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |
|||
Vicat Softening Point | 52.0 °C | 126 °F | ISO 306 |
Total Evatane® 24 - 03 HDPE vinyl acetate copolymer, blown film, injection molding
(discontinued **) EVA Copolymer made by high pressure tubular process. Temperature profile (°C) for injection molding: 130 to 160.Information provided provided by Total Petrochemicals.Total Petrochemicals includes f.. |
|||
Vicat Softening Point | 52.0 °C | 126 °F | 1000g; ASTM D-1525 |
ExxonMobil Escorene® LD-740 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty film and compounding applications. Outstanding heat sealability along with excellent strength pr.. |
|||
Vicat Softening Point | 52.0 - 87.0 °C | 126 - 189 °F | Average value: 80.0 °C Grade Count:123 |
Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Vicat Softening Point | 52.0 - 192 °C | 126 - 378 °F | Average value: 110 °C Grade Count:62 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Vicat Softening Point | 52.0 - 54.0 °C @Load 5.00 kg |
126 - 129 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RST 0447/1 Rigid PVC, Extrusion Lead Free Extrusion transparent films |
|||
Vicat Softening Point | 52.0 °C | 126 °F | B (50N); ISO 306 |
Borealis Daplen™ KSR4525 Polypropylene Reactor Elastomer Modified Daplen KSR4525 is a reactor elastomer modified polypropylene intended for injection molding. Daplean KSR4525 is a material with excellent impact/stiffness ratio. The grade is available in natural .. |
|||
Vicat Softening Point | 52.0 °C | 126 °F | B (50N); ISO 306 |
Borealis Daplen™ EE260AE Scratch Resistant Polypropylene Compound Daplen EE206AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE206AE is optimized to provide excellent scratch resistance on gained and unpai.. |
|||
Vicat Softening Point | 52.0 °C | 126 °F | ASTM D1525 |
DuPont Elvax® 3190 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion 25 wt% Vinyl Acetate.Elvax® 3190 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Vicat Softening Point | 52.0 °C | 126 °F | |
Covestro Desmopan® 460 Thermoplastic Polyurethane Desmopan 460 is a TPU on the basis of a special ester.Applications: Bearing shells, gear wheels, seals, cable connectors.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience w.. |
|||
Vicat Softening Point | 52.0 °C | 126 °F | ASTM D1525, ISO 306 |
DuPont™ Bynel® 21E787 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Vicat Softening Point | 52.2 °C | 126 °F | ASTM D1525 |
ExxonMobil Vistamaxx™ 6102 Propylene-based Elastomer Product Description: Vistamaxx 6102 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Catalyst Technology. It has excellent elastomeric properties, i.. |
|||
Vicat Softening Point | 52.2 °C | 126 °F | ASTM D1525 |
ExxonMobil Vistamaxx™ 6102FL Propylene-based Elastomer - Performance Film Product Description: Vistamaxx 6102FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution. It is produced us.. |
|||
Vicat Softening Point | 52.2 °C | 126 °F | ASTM D1525 |
ExxonMobil Escorene™ FL 01418 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 01418 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. FL 01418 is an excellent sealing materi.. |
|||
Vicat Softening Point | 52.0 °C | 126 °F | 50°C/hr; 50N |
Arkema Group Appryl® CZN 0525 Polypropylene, 25% Talc Filled Compound of a PP copolymer modified with EPR and 25% talc. This grade has been specially developed for interior trim applications, that required an excellent impact test associated with a high modul.. |
|||
Vicat Softening Point | 52.0 °C | 126 °F | ISO 306 |
Arkema Group OREVAC® 18390 Maleic Anhydride Modified Polyethylene OREVAC® 18390 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Vicat Softening Point | 52.0 °C | 126 °F | 50°C/hr; 50N |
Arkema Group Appryl® CZT 1030 Polypropylene, 30% Talc/Mica Filled Compound of a PP copolymer modified with EPR and 30% of a mixture of talc and mica. This grade has been specially developed for exterior automotive applications, that required an excellent thermal d.. |
|||
Vicat Softening Point | 52.0 °C | 126 °F | 50°C/hr; 50N |
Arkema Group Appryl® CZU 0525 Polypropylene, 25% Talc Filled Compound of a PP copolymer modified with EPR and 25% talc. This grade has been specially developed for exterior trim automotive applications, that required an excellent impact test associated with a.. |
|||
Vicat Softening Point | 52.0 - 117 °C | 126 - 243 °F | Average value: 89.3 °C Grade Count:151 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Vicat Softening Point | 52.2 °C | 126 °F | ASTM D1525 |
Lubrizol ESTANE® 58224 Ester Based Thermoplastic Polyurethane Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Vicat Softening Point | 52.0 °C | 126 °F | ASTM D1525 |
DuPont Elvax® 3190LG Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
(discontinued **) 25 wt% Vinyl Acetate.Elvax® 3190 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |