Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 39.0 °C
102 °F
1000g; ASTM D-1525
ExxonMobil Optema® TC-221 Ethylene Methyl Acrylate for Compounding  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.27% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be used for making alloys, blends, and compounds, or be injection molded where..
Vicat Softening Point 39.0 °C
102 °F
B (50N); ISO 306
Borealis Daplen™ ED213AE TPO Compound
Daplen ED213AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen ED213AE is a material with excellent impact/ stiffness ratio. Thanks to its low..
Vicat Softening Point 39.0 °C
102 °F
ASTM D1525
Dow Engage® 8100 Polyolefin Elastomer
Description: Engage® 8100 polyolefin elastomer is an ethyleneoctene copolymer that has excellent flow characteristics and performs well in a wide range of general purpose thermoplastic elastomer ap..
Vicat Softening Point 39.0 °C
102 °F
ASTM D1525
Dow Engage® 8107 Polyolefin Elastomer
Description: Engage® 8107 polyolefin elastomer is a loose talc surface coated ethylene-octene copolymer. The talc is untreated and has a nominal 1µm particle size. This product offers the exceptio..
Vicat Softening Point 39.0 °C
102 °F
ASTM D1525
Dow Engage® 8150 Polyolefin Elastomer
Description: Engage® 8150 and Engage® 8157 polyolefin elastomers are ethylene-octene copolymers that have excellent flow characteristics and provide good impact properties in blends with polypropy..
Vicat Softening Point 39.0 °C
102 °F
ASTM D1525
Dow Engage® 8157 Polyolefin Elastomer
Description: Engage® 8157 polyolefin elastomer is a loose talc surface coated ethylene-octene copolymer. The talc is untreated and has a nominal 1µm particle size. This product offers the exceptio..
Vicat Softening Point 39.0 - 71.0 °C
102 - 160 °F
Average value: 52.1 °C Grade Count:7
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Compounding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Compounding Grade". Each property range of values reported is minimu..