Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 86.0 °C | 187 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Geloy XTWE280 ASA (Europe-Africa-Middle East) Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Geloy FXTW30CP ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Geloy XTWE280 ASA (Asia Pacific) Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | >= 86.0 °C | >= 187 °F | At 1 kg; ASTM D1525 |
Iran Petrochemical (PCC) Tabriz 3630/1 High Impact Polystyrene
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
Eastman E6838-889P Polyethylene
(discontinued **) Polyethylene E6838-889P is a formulation suggested for extrusion coating applications and has been used successfully in compounding. This product may be used for holding food during cooking.Applicat.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
ICO Polymers ICOFLOâ„¢ 510-5061 1200 Micron LDPE Powder Description: ICOFLO 510-5061 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Vicat Softening Point | 86.0 °C @Load 5.00 kg |
187 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical LI931 Extrusion ASA Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
LyondellBasell Petrothene® NA870252 Low Density Polyethylene ApplicationsPETROTHENE NA 870-252 exhibits an excellent balance of toughness and softness, with excellent dimensional stability. Typical applications include caps and closures, housewares, toys, co.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ISO 306 |
Lucobit Lucofin® 1400HN Powder Ethylene Butyl Acrylate Lucofin 1400HN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN Powder is softer and more flexible than ethy.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 50°C/h; 50N; 10x10x4mm; ISO 306/B50 |
SYNTHOS Krasten® 154 General Purpose Polystyrene Improved heat resistance, very good rheological properties.Examples of Application:Injection moulding – dishes, jars, Petri dishes, screw caps.Extrusion – blends with high impact polystyre.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | Phr = 0 |
Shandong Rike Chemical HELIâ„¢ HL-56 Weather-resistance Acrylic Impact Modifier (AIM) Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | Phr = 0 |
Shandong Rike Chemical HELIâ„¢ HL-57 Weather-resistance Acrylic Impact Modifier (AIM) Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
DuPont Bynel® 4208 Anhydride-Modified LDPE Adhesive Resin Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process .. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM-D1525 |
Polyram RamShine PV507 ABS, Flame Retardant Flame retardant ABS for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 1kg load; ASTM D1525 |
Eastman DuraStar DS1900HF Polymer, Natural Durastar DS1900HF polymer is a high flow grade of Durastar . Durastar DS1900HF flow lengths are increased 20-40% relative to Durastar DS1000 as shown by spiral flow testing. Other outstanding featur.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 1kg load; ASTM D1525 |
Eastman DuraStar DS1910HF Polymer, Natural Durastar DS1910HF polymer is a high flow grade of Durastar that contains a mold release. Durastar DS1910HF flow lengths are increased 20-40% relative to Durastar DS1010 as shown by spiral flow testi.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 1kg load; ASTM D1525 |
Eastman DuraStar MN630 Polymer, Natural Durastar Polymer MN630 has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN630 has very .. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 1kg load; ASTM D1525 |
Eastman DuraStar MN631 Polymer, Natural Durastar Polymer MN631 contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing char.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 1kg load; ASTM D1525 |
Eastman Eastar AN011 Copolyester Eastar AN011 copolyester is a high flow product. Eastar AN011 flow lengths are increased 20-40% relative to Eastar AN001 as shown by spiral flow testing. Other outstanding features of Eastar are eas.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
Eastman Spectar® Clear Copolyester for Thermoforming Applications:Decorative Light-Transmitting PanelsHeavy gauge sheet displaysKey Attributes:Easy to print and decorateExcellent clarityExcellent thermoforming characteristicsGood chemical resistanceOd.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | Loading 1, Rate A; ASTM D1525 |
Chevron Phillips Marlex® 1003 LDPE Injection Molding Resin Resin Type: HomopolymerCharacteristics: Excellent flexibilityExcellent flowModerate mold releaseGood warpage resistanceApplications: HousewaresTamper evident, snap-on capsWine bottle sleeve capsInfo.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 50N; ISO 306 |
Denka TP-802 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
Dow AFFINITY™ PL 1880G Polyolefin Plastomer (POP) AFFINITY™ PL 1880G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal packagi.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
Dow Engage® 8480 Polyolefin Elastomer Description: Engage® 8480 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in footwear applications and profile extrusion of tubing and hoses. It has good clari.. |
|||
Vicat Softening Point | 86.0 °C @Load 1.02 kg |
187 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem F 7018 LDPE Extrusion Coating Polyethylene LDPE F 7018 is a low-density polyethylene and has excellent processability and sealability at low temperatures. It does not contain additives. Its applications include: extrusion coating; and injec.. |
|||
Vicat Softening Point | 86.0 °C @Load 1.02 kg |
187 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem F7018 LDPE Injection Molding Polyethylene F7018 is a low-density polyethylene with excellent processability and sealability at low temperatures. It does not contain additives. Its applications include: extrusion coating, injection molding .. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
Huntsman Rexell® L2101 Injection Molding LLDPE
(discontinued **) Linear-low very low density copolymer, injection molding, FDA compliant.Features: High flow, flexible with excellent environmental stress crack (ESCR), and warpage resistance.Applications: Fitments,.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
DuPont Nucrel® 0910HS-SR Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating
(discontinued **)< 8.7 wt% Methacrylic Acid.Nucrel® 0910HS-SR is an ethylene-methacrylic acid copolymer resin available for use in conventional and coextrusion coating equipment designed to process polyethylene resin.. |