Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525 |
Plaskolite PETG Mirror Sheet Versatile fabrication properties with good impact strength, good design flexibility, and speed of fabrication.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Vicat Softening Point | 82.0 °C @Load 1.00 kg |
180 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Greenflex® FL 25 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FL 25 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FL 25 show good optical properties and excellent sealability.Main Applications: .. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 241 Rigid PVC, Extrusion Various profiles |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 425/R Rigid PVC, Extrusion Shiny electric channels |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RK 218 Rigid PVC, Extrusion Lead Free Rolling shutters |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RK 325 Rigid PVC, Extrusion Lead Free Verticle curtains |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RK 330 Rigid PVC, Extrusion Lead Free Profiles |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525 |
ICO Polymers ICOFLOâ„¢ 510-5018 400 Micron LDPE Powder Description: ICOFLO 510-5018 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525 |
ICO Polymers ICOFLOâ„¢ 510-5053 500 Micron LDPE Powder Description: ICOFLO 510-5053 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ISO 306B |
Lucite International Diakon® ST45G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ISO 306 |
Stir SpA HE 625 A (PVC) Application: Economic medium shock resistantInformation provided by STIR SpA |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525 |
SK Chemicals SKYTHANE® 180A R series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525 |
DuPont Elvax® 3135X Ethylene-Vinyl Acetate Copolymer Resin for Thin Blown 12 wt% Vinyl Acetate.Elvax® 3135X is an extrudable, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525, ISO 306 |
DuPont Elvax® 3135XZ Ethylene Vinyl Acetate DuPont™ Elvax® 3135XZ is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.Applicati.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525 |
Lubrizol Estane® R180A Thermoplastic Polyurethane Type: Estane® R180A is a Shore 83A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provi.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525, ISO 306 |
DuPont™ Bynel® 41E865 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds R 316/AS Rigid PVC, Extrusion Antistatic profiles |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 121 Rigid PVC, Extrusion Electric pipes |
|||
Vicat Softening Point | 82.0 °C | 180 °F | |
BASF Polystyrol® 432 B Impact Grade Polystyrene (Europe) Very easy-flowing, low impact grade for parts with unfavorable flow path/wall-thickness ratios.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | 50°C/hr; 50N |
Polimeri Europa EDISTIR SRL550 High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,E,083-12-07-18 High impact, easy flow polystyrene with good elasticity at low temperatures. Used for sheet extrusion and .. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 224 Rigid PVC, Extrusion Various profiles |
|||
Vicat Softening Point | 82.0 °C | 180 °F | 1000g; ASTM D-1525 |
ExxonMobil Escorene® LD-712 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt, 10% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness... |
|||
Vicat Softening Point | 82.0 °C | 180 °F | 50°C/h; 50N; 10x10x4mm; ISO 306/B50 |
SYNTHOS Krasten® 336M High Impact Polystyrene Easy flow grade. Processed by injection moulding of intricate and thin-walled products that enables high production output.Synthos was formerly known as Kaucuk. All information provided by Synthos. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525, ISO 306 |
DuPont Elvax® 760Q Ethylene Vinyl Acetate DuPont™ Elvax® 760W is a low BHT anti-oxidant ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications: Elvax® 760Q resins can be used for the following applicati.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525, ISO 306 |
DuPont Elvax® 880 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 880 is an ethylene-vinyl acetate copolymer resin containing slip and anti-block additives for use in industrial applications.Applications: Elvax® 880 resins can be used for the fo.. |