Thermal Properties Metric English Comments
Vicat Softening Point 35.0 - 165 °C
95.0 - 329 °F
Average value: 103 °C Grade Count:94
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
Vicat Softening Point 35.0 - 99.0 °C
95.0 - 210 °F
Average value: 76.9 °C Grade Count:41
Overview of materials for Styrene-Butadiene Copolymer, SBC
This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values ..
Vicat Softening Point 35.0 °C
95.0 °F
VST/A/120; ISO 306
Styrolution Styroflex® 2G 66 SBC
Description: Styroflex® 2G 66 is a styrene-butadiene block copolymer (SBC) with the properties of a thermoplastic elastomer (S-TPE). Styroflex® 2G 66 is the only S-TPE with a styrene content o..
Vicat Softening Point 35.0 °C
95.0 °F
(50 °C/h / 50N) - B/50; ISO 306
Styrolution Styrolux 3G55 SBC
Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex..
Vicat Softening Point 35.0 °C
95.0 °F
ASTM D1525
Lubrizol ESTANE® 5719 Ester Based Thermoplastic Polyurethane
Features: High tensile strength, low temperature flexibility, and high adhesion to various substrates such as PET, PVC, and various fabrics.Uses: Fabric coating and audio tape binder, inks and solut..
Vicat Softening Point 35.0 °C
95.0 °F
BASF Novolen® 2900 NC Polypropylene