Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 243 °C | 469 °F | B/50; ISO 306 |
Eurostar Staramide A28K PA66, Heat Stabilized, Injection Molding Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 243 °C | 469 °F | B/50; ISO 306 |
Eurostar Staramide A28N PA66, Nucleated, Injection Molding Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 243 °C | 469 °F | B/50; ISO 306 |
Eurostar Staramide R1000 PA66, Injection Molded Staramide R1000 is an Unreinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |