Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 193 °C | 379 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 193 °C | 379 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 193 °C | 379 °F | ASTM D1525 |
Samyang Triel® 5600 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5600 is an extrusion grade.Information provided by Samyang. |
|||
Vicat Softening Point | 193 °C | 379 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL PX500 PPE (Asia Pacific) Noryl PX500 is an unfilled modified polyphenylene ether resin capable of multiple conversion routes. This resin is designed for lower odor during conversion than many standard modified PPE resins. .. |
|||
Vicat Softening Point | 193 °C | 379 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Vicat Softening Point | 193 °C | 379 °F | ASTM D1525 |
Toyobo PELPRENE™ S3001 Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Vicat Softening Point | 193 °C | 379 °F | |
Covestro Apec® HT KU 1-9361 High-Heat Polycarbonate Transparent and opaque shades possible.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated .. |
|||
Vicat Softening Point | 193 °C | 379 °F | ASTM D1525 |
Toyobo PELPRENE™ S3002 Polyester TPE, Ultra Heat-resistant Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo. |