Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0250 GPa @Temperature 200 °C |
3.63 ksi @Temperature 392 °F |
ISO 6721 |
BASF Ultrason S 2010 G4 20% Glass Filled PSU Ultrason S 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
Shear Modulus | 0.0250 GPa @Temperature 200 °C |
3.63 ksi @Temperature 392 °F |
ISO 6721 |
BASF Ultrason S 2010 G6 30% Glass Filled PSU Ultrason S 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
Shear Modulus | 0.0250 GPa @Temperature 200 °C |
3.63 ksi @Temperature 392 °F |
ISO 6721 |
BASF Ultrason S 2010 PSU Ultrason S 2010 is an unreinforced, medium viscosity standard injection molding PSU grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Shear Modulus | 0.0250 GPa @Temperature 200 °C |
3.63 ksi @Temperature 392 °F |
ISO 6721 |
BASF Ultrason S 3010 PSU Ultrason S 3010 is an unreinforced, higher viscosity injection molding and extrusion PSU grade, tougher and with improved chemical resistance. It conforms to FDA requirements of 21 CFR 177.1655. |