PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Shear Modulus 34.0 GPa

@Temperature 300 °C
4930 ksi

@Temperature 572 °F
PEAK Werkstoff DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Shear Modulus 34.0 GPa

@Temperature 150 °C
4930 ksi

@Temperature 302 °F
PEAK Werkstoff DISPAL S226 Aluminum Alloy, AlSi30CuMg, Condition T6
Heat Treatment Condition T6 (Quench in water at RT)abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of p..
Shear Modulus 34.0 GPa

@Temperature 200 °C
4930 ksi

@Temperature 392 °F
PEAK Werkstoff DISPAL S226 Aluminum Alloy, AlSi30CuMg, Condition T6
Heat Treatment Condition T6 (Quench in water at RT)abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of p..
Shear Modulus 34.0 GPa

@Temperature 100 °C
4930 ksi

@Temperature 212 °F
Condition T6x (Quench in water at RT)
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6
Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo..
Shear Modulus 34.0 GPa

@Temperature 100 °C
4930 ksi

@Temperature 212 °F
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x
Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all..
Shear Modulus 34.0 GPa

@Temperature 300 °C
4930 ksi

@Temperature 572 °F
PEAK Werkstoff DISPAL S250 Aluminum Alloy, AlSi20Fe5Ni2, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Shear Modulus 34.0 GPa

@Temperature 100 °C
4930 ksi

@Temperature 212 °F
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Shear Modulus 34.0 GPa

@Temperature 100 °C
4930 ksi

@Temperature 212 °F
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..