Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 40.0 MPa @Temperature 129 °C |
5800 psi @Temperature 264 °F |
Short Beam, Wet |
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber Information provided by HexCel |
|||
Shear Strength | 40.0 MPa @Temperature 60.0 °C |
5800 psi @Temperature 140 °F |
0°, Interlaminar, Conditioning: 60°C-90% RH; ASTM D2344 |
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, HTA Fiber Designation: C193PW, Plain weaveInformation provided by HexCel |
|||
Shear Strength | 40.0 MPa @Temperature 71.1 °C |
5800 psi @Temperature 160 °F |
Lap Shear |
Hexcel® Redux® 308A-NA Modified epoxy film adhesive Redux 308A-NA is a high-strength, flow-controlled film adhesive with flexible cure schedules at 300°F or 350°F. Redux 308A-NA contains glass beads that give good flow control. It is suitable for m.. |
|||
Shear Strength | 40.0 MPa @Temperature 60.0 °C |
5800 psi @Temperature 140 °F |
0°, Interlaminar, Conditioning: 60°C-90% RH; ASTM D2344 |
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, AS4-C Fiber Designation: C193PW, Plain weaveInformation provided by HexCel |