Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 2.07 MPa @Temperature 0.000 °C |
300 psi @Temperature 32.0 °F |
Tensile, Al/Al lap joint; cured 7 days @ 25°C |
Abatron AboCast 8110-1/AboCure 8110-3 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |
|||
Shear Strength | 2.07 MPa @Temperature 82.0 °C |
300 psi @Temperature 180 °F |
Overlap |
3M Scotch-Weld™ 1838L B/A Two-Part Structural Adhesive Multi-purpose and Rigid bondsInformation provided by 3M |
|||
Shear Strength | 2.07 MPa @Temperature -53.0 °C |
300 psi @Temperature -63.4 °F |
Aluminum Overlap |
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive 3M™ Scotch-Weld™ Non-Metallic Filled is a non-metal filled version of Scotch-Weld adhesive 2214 regular. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a pa.. |
|||
Shear Strength | 2.07 MPa @Temperature 82.0 °C |
300 psi @Temperature 180 °F |
Overlap |
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 2.07 MPa @Temperature 82.0 °C |
300 psi @Temperature 180 °F |
Overlap, Etched Aluminum |
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 2.07 MPa @Temperature 82.0 °C |
300 psi @Temperature 180 °F |
Overlap, Abraded and Solvent Wiped Al |
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 2.07 MPa @Temperature 82.0 °C |
300 psi @Temperature 180 °F |
Overlap, ABS |
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 2.07 MPa @Temperature 82.0 °C |
300 psi @Temperature 180 °F |
Overlap |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 2.07 MPa @Temperature 82.0 °C |
300 psi @Temperature 180 °F |
Overlap, Etched Aluminum |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 2.07 MPa @Temperature 82.0 °C |
300 psi @Temperature 180 °F |
Overlap, Abraded and Solvent Wiped Al |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 2.07 MPa @Temperature 82.0 °C |
300 psi @Temperature 180 °F |
Overlap, ABS |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 2.07 MPa @Temperature 82.0 °C |
300 psi @Temperature 180 °F |
Overlap |
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 2.07 MPa @Temperature 82.0 °C |
300 psi @Temperature 180 °F |
Overlap, Etched Aluminum |
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 2.07 MPa @Temperature 82.0 °C |
300 psi @Temperature 180 °F |
Overlap, Abraded and Solvent Wiped Al |
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 2.07 MPa @Temperature 82.0 °C |
300 psi @Temperature 180 °F |
Overlap, ABS |
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 2.07 MPa @Temperature 82.0 °C |
300 psi @Temperature 180 °F |
Overlap |
3M Scotch-Weld™ DP270 Black Structural Adhesive Rigid potting compound, Non-corrosiveInformation provided by 3M |
|||
Shear Strength | 2.07 - 2.41 MPa @Temperature 82.0 °C |
300 - 350 psi @Temperature 180 °F |
Overlap Al/Al (etched); ASTM D1002-72 |
3M Scotch-Weld™ DP270 Black Structural Adhesive Rigid potting compound, Non-corrosiveInformation provided by 3M |
|||
Shear Strength | 2.07 MPa @Temperature 82.0 °C |
300 psi @Temperature 180 °F |
Overlap |
3M Scotch-Weld™ DP270 Clear Structural Adhesive Rigid potting compound, Non-corrosiveInformation provided by 3M |
|||
Shear Strength | 2.07 - 2.41 MPa @Temperature 82.0 °C |
300 - 350 psi @Temperature 180 °F |
Overlap Al/Al (etched); ASTM D1002-72 |
3M Scotch-Weld™ DP270 Clear Structural Adhesive Rigid potting compound, Non-corrosiveInformation provided by 3M |