Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 76.5 MPa @Temperature 150 °C |
11100 psi @Temperature 302 °F |
JIS K7214 |
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Shear Strength | 76.5 MPa @Temperature 232 °C |
11100 psi @Temperature 450 °F |
Short Beam; 1608 Hrs |
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber Thermal Aging at 232°C; Composition T300 Fiber, 6K, UD Tape - 148 g/m2; Laminate Physicals: 32.7% Resin content, 60.0% Fiber volumeInformation provided by HexCel |
|||
Shear Strength | 76.5 MPa @Temperature 232 °C |
11100 psi @Temperature 450 °F |
Short Beam; 2010 Hrs |
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber Thermal Aging at 232°C; Composition T300 Fiber, 6K, UD Tape - 148 g/m2; Laminate Physicals: 32.7% Resin content, 60.0% Fiber volumeInformation provided by HexCel |
|||
Shear Strength | 76.4 MPa @Temperature 23.0 °C |
11100 psi @Temperature 73.4 °F |
ILSS; prEN2563 |
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/42%/G1094/1000 Fiber: T800H 6K, 5H Satin weave, 290 g/m2Information provided by HexCel |