Shear Strength 13.1 MPa

@Temperature 204 °C
1900 psi

@Temperature 400 °F
ASTM D732
Greene Tweed Avalon® 1 PTFE
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin..
Shear Strength 13.1 MPa

@Temperature 93.3 °C
1900 psi

@Temperature 200 °F
Lap Shear
Hexcel® Redux® 335K Adhesive film for bonding metallic and composite components (0.06 psf)
Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a..
Shear Strength 13.1 MPa

@Temperature 82.0 °C
1900 psi

@Temperature 180 °F
with Scotch-Weld EW-5000; ASTM D1002-10
3M Scotch-Weld™ EC-2815 B/A FR Epoxy Adhesive
3M Scotch-Weld Epoxy Adhesive EC-2815 B/A FR is a two-component epoxy adhesive with cure at room temperature or with additional heat to form a tough, impact-resistant bond. It has excellent adhesion..
Shear Strength 13.1 MPa

@Time 86400 sec
1900 psi

@Time 24.0 hour
Overlap, PVC
3M Scotch-Weld™ EZ250030 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th..
Shear Strength 13.1 MPa

@Temperature 23.0 °C
1900 psi

@Temperature 73.4 °F
Overlap, PVC, Substrate Failure