Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Greene Tweed Avalon® 1 PTFE

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Molded
Manufacturer Greene Tweed
Trade Name Avalon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed Avalon® 1 PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin to reinforced, exhibit low friction while being chemically inert. Avalon thermoplastics can be custom designed to for each unique application.Information provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 2.18 g/cc
2.18 g/cc
ASTM D792
Deformation 7.0 %
7.0 %
2000 psi 78°F; ASTM D621
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM D1457
Elongation at Break 350 %
350 %
ASTM D1457
Shear Strength 13.1 MPa

@Temperature 204 °C
1900 psi

@Temperature 400 °F
ASTM D732
14.5 MPa

@Temperature 149 °C
2100 psi

@Temperature 300 °F
ASTM D732
14.8 MPa

@Temperature 93.3 °C
2150 psi

@Temperature 200 °F
ASTM D732
16.5 MPa

@Temperature 65.6 °C
2400 psi

@Temperature 150 °F
ASTM D732
20.7 MPa

@Temperature 37.8 °C
3000 psi

@Temperature 100 °F
ASTM D732
25.5 MPa

@Temperature 26.7 °C
3700 psi

@Temperature 80.0 °F
ASTM D732
Coefficient of Friction, Dynamic 0.080
0.080
33.3 psi @ 150 fpm
Coefficient of Friction, Static 0.050
0.050
33.3 psi
K (wear) Factor 5040 x 10-8 mm³/N-M
2500 x 10-10 in³-min/ft-lb-hr
Descriptive Properties Value Comments
Color White