Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 11.0 MPa @Temperature 150 °C |
1600 psi @Temperature 302 °F |
Lap Shear; Cured 5 days at 23°C; Substrate: 2024 T3 Aluminum Alloy (CSA pretreated, Unprimed); EN2243-1 |
Hexcel® Redux® 870 A/B Two Component Shimming and Potting Epoxy Paste Adhesive Redux 870 A/B is a two component high performance epoxy paste adhesive, ideal for use as a Liquid Shim or for potting applications. This high temperature performing thixotropic adhesive has been spe.. |
|||
Shear Strength | 11.0 MPa @Temperature 177 °C |
1600 psi @Temperature 351 °F |
Short Beam |
Hexcel® F161 Epoxy Resin, 285 Kevlar Fabric Hexcel designation: 285-38"-F161; Fiber: Kev. 49 1140Information provided by HexCel |
|||
Shear Strength | 11.0 MPa @Temperature 93.3 °C |
1600 psi @Temperature 200 °F |
Lap Shear |
Hexcel® Redux® 335M Adhesive film for bonding metallic and composite components (0.03 psf) Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a.. |
|||
Shear Strength | 11.0 MPa @Temperature 80.0 °C |
1600 psi @Temperature 176 °F |
Double Lap Shear; Dry; 60 min @ 120°C; Hexcel IS202 |
Hexcel® Redux® 840 One-part Foaming Epoxy Paste Adhesive Redux® 840 is a black one-part, foaming, epoxy paste adhesive that is thixotropic.Features: Provides a shear-carrying connection across any discontinuities in bonded sandwich panels; Maximum servic.. |
|||
Shear Strength | 11.0 MPa @Temperature 23.0 °C |
1590 psi @Temperature 73.4 °F |
Overlap, Polycarbonate |
3M Scotch-Weld™ TE040 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |