Mechanical Properties Metric English Comments
Flexural Strength 155 MPa

@Temperature 23.0 °C
22500 psi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK 600G Polyetheretherketone  (discontinued **)
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta..
Flexural Strength 155 MPa

@Strain 6.70 %
22500 psi

@Strain 6.70 %
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® BKV 130 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified
PA 6, 30% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Flexural Strength 155 MPa

@Strain 4.00 %
22500 psi

@Strain 4.00 %
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant
PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS.
Flexural Strength 155 MPa

@Temperature 80.0 °C
22500 psi

@Temperature 176 °F
Practical Use (Water Absorption 0.8%); ASTM-D790
Toyobo GLAMIDE® T-663G50A MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 155 MPa

@Temperature -40.0 °C
22500 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 1.9%); ASTM-D790
Toyobo GLAMIDE® TY-502NZ 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 155 MPa

@Temperature -40.0 °C
22500 psi

@Temperature -40.0 °F
ASTM D790
BASF Ultramid® 8202 L Intermediate PA6 (Conditioned)
Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai..
Flexural Strength 155 MPa

@Temperature 23.0 °C
22500 psi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK 650G Polyetheretherketone