Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 165 MPa @Temperature 23.0 °C |
23900 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 450G General Purpose Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac.. |
|||
Flexural Strength | 165 MPa @Temperature 23.0 °C |
23900 psi @Temperature 73.4 °F |
50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66
(Unverified Data**) Zytel® 70G25HSL NC010 is a 25% glass fiber reinforced, heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Strength | 165 MPa @Thickness 1.57 mm |
24000 psi @Thickness 0.0620 in |
CW; ASTM D790 |
Industrial Laminates/Norplex NP664 Paper Base Laminate Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062.. |
|||
Flexural Strength | 165 MPa @Temperature -40.0 °C |
23900 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 2.3%); ASTM-D790 |
Toyobo GLAMIDE® T-422-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 165 MPa @Temperature 23.0 °C |
23900 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |
|||
Flexural Strength | 165 MPa @Temperature 23.0 °C |
23900 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac.. |