Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 118 kN/m | 672 pli | 50mm/min, at Break; ASTM D624 |
LG Chemical KEYFLEX BT 1040D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Tear Strength | 118 kN/m | 672 pli | 50mm/min, at Break; ASTM D624 |
LG Chemical KEYFLEX BT 1140D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Tear Strength | 118 kN/m | 672 pli | ASTM D624 |
Kolon ELLAS K-585A Caprolactone Based Thermoplastic Polyurethane ApplicationsInjectionIndustry Parts Information provided by API-Kolon. |
|||
Tear Strength | 118 kN/m | 672 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® S392A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tear Strength | 118 kN/m | 672 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® X590A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tear Strength | 118 kN/m | 672 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® 590A X series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tear Strength | 118 kN/m | 672 pli | Die C; ASTM D624 |
Lubrizol Estane® S392A Thermoplastic Polyurethane Type: Estane® S392A is a Shore 93A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion, Blow .. |
|||
Tear Strength | 118 kN/m | 672 pli | Die C; ASTM D624 |
Lubrizol Estane® CS195A Thermoplastic Polyurethane Type: Estane® CS195A is a Shore 95A, polyester grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf.. |
|||
Tear Strength | 118 kN/m | 672 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® 392A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |