SK Chemicals SKYTHANE® 590A X series Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer SK Chemicals
Trade Name SKYTHANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SK Chemicals SKYTHANE® 590A X series Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical property. It is widely used for automotive parts and various industrial parts.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Hardness, Shore D 44
44
ASTM D2240
Tensile Strength, Ultimate 53.9 MPa
7820 psi
ASTM D412
Tensile Strength, Yield 9.81 MPa

@Strain 100 %
1420 psi

@Strain 100 %
ASTM D412
19.1 MPa

@Strain 300 %
2770 psi

@Strain 300 %
ASTM D412
Elongation at Break 650 %
650 %
ASTM D412
Resilience 40
40
by vertical rebound; ASTM D2632
Tear Strength 118 kN/m
672 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 40
40
H18 Wheel; 1000g load; ASTM D1044
Thermal Properties Metric English Comments
Vicat Softening Point 110 °C
230 °F
ASTM D1525