Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 10.2 kN/m | 58.2 pli | ISO 34 Method C |
Rogers Corporation Bisco® A2 Sound Barrier Engineered Solid Silicone Mass Layer, Sound Barrier BISCO® A2 Sound Barrier is a solid silicone rubber engineered to meet demanding requirements for flammability, smoke density and toxicity. A2 is used to block the transmission of sound and demonst.. |
|||
Tear Strength | 10.2 kN/m | 58.2 pli | ASTM D624 |
Teknor Apex Uniprene® UN-2023 Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tear Strength | 10.2 kN/m | 58.2 pli | ASTM D624 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2325 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |