Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 0.300 kN/m | 1.71 pli | |
Fujipoly Industries Sarcon® 30T Thin-Film TR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Tear Strength | 0.300 kN/m | 1.71 pli | |
Fujipoly Industries Sarcon® 30U Thin-Film UR Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Tear Strength | 0.300 kN/m | 1.71 pli | |
Fujipoly Industries Sarcon® 45H Thin-Film HR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Tear Strength | 0.300 kN/m | 1.71 pli | Split Tear Strength, ASTM D3574-F |
Covestro Bayfill® 312 Polyurethane Semi-Rigid Foam, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |