Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 87.0 - 140 kN/m | 496 - 799 pli | Average value: 109 kN/m Grade Count:12 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade". Each property range of values reported is mini.. |
|||
Tear Strength | 87.0 kN/m | 496 pli | Die C, 2 in/min; D1004 |
Phillips Sumika Marlex® CHP-035 Thermoplastic Polyolefin
(discontinued **) Applications: Painted air-bag coversSoft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. |
|||
Tear Strength | 87.0 kN/m | 497 pli | Type C; ASTM D624 |
LG Chemical LC100 Polyolefin Elastomer Features: Excellent toughness with flexible performance, High clarity and low temperature sealability. High performance in footwear applicationApplication: Polymer modification, Shoe sole, Film coex.. |
|||
Tear Strength | 87.0 kN/m | 496 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-1180 Polyester Based TPU Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 87.0 kN/m | 496 pli | Die C; ASTM D624 |
Covestro Bayflex® 110-50 CM Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |