Mechanical Properties Metric English Comments
Tear Strength 47.0 kN/m
268 pli
Die B,post cured- 2 hours at 200°C; ASTM D624
Multibase SILASTIC® 7-6840 Dow-Corning Biomedical Grade Liquid Silicone Rubber
Information provided by Multibase
Tear Strength 47.0 kN/m
268 pli
as molded; Die B
Multibase SILASTIC® C7-4565 CADOX TS-50S Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tear Strength 47.0 kN/m
268 pli
Die B
Momentive Performance Materials TUFELâ„¢ II 94505 Low Volatile Extrusion Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 47.0 kN/m
268 pli
Die B
Momentive Performance Materials TUFELâ„¢ II 94506 Low Volatile Extrusion Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 47.0 kN/m
268 pli
ASTM D624
UBE UBEPOL BR100 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
Tear Strength 47.0 kN/m
268 pli
ASTM D624
UBE UBEPOL BR150 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
Tear Strength 47.0 kN/m
268 pli
ASTM D2240
UBE UBEPOL BR153A Oil-Extended BR Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
Tear Strength 47.0 kN/m
268 pli
ASTM D624
UBE UBEPOL VCR150 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel..
Tear Strength 47.0 kN/m
268 pli
GB/T 529
Chengdu Polyster 7500 General Grade TPV
Information provided by Chengdu Polyster Co., Ltd.
Tear Strength 47.0 kN/m
268 pli
Die C; ASTM D 624
CPT C-Flex® R70-089 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Tear Strength 47.0 kN/m
268 pli
73°C, Die C; ASTM D624
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer
A hard, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Tear Strength 47.0 kN/m
268 pli
ISO 34-B
AlphaGary Evoprene™ 032 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Tear Strength 47.0 kN/m
268 pli
ASTM D1004
Bayshore Vinyl Compounds BVC 1100-65 Clear PVC Compound
BVC 1100-65 is a clear flexible PVC compound produced with FDA sanctioned ingredients. It is recommended for use in applications for the medical, food and beverage industries. This material offers..
Tear Strength 47.0 kN/m
268 pli
Parallel to flow; ISO 34-B
AlphaGary Evoprene™ LF 6156 Automotive Thermoplastic Elastomer
Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab..
Copyright © lookpolymers.com All Rights Reserved